Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | <= 70.0 MPa | <= 10200 psi | ISO/R527 |
Polykemi AB POLYform POM C M90 GF10 Polyoxymethylene Information provided by Polykemi AB |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 134R PC (Europe-Africa-Middle East) LEXAN 134R is a high viscosity grade especially suited for injection blow moulding. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported.. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 243R PC (Europe-Africa-Middle East) LEXAN 243R is a medium viscosity multi purpose UV stabilized grade and contains release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® 4401R PPC+PC (Europe-Africa-Middle East) LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXD103 PC (Asia Pacific) FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the .. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXD103 PC (Europe-Africa-Middle East) FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the .. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXD103R PC (Europe-Africa-Middle East) FXD103R is a Light Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect propert.. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXE144H PC FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe.. |
|||
Tensile Strength at Break | 70.0 MPa @Temperature 23.0 °C |
10200 psi @Temperature 73.4 °F |
ISO 527-2/5 |
PolyOne Bergamid™ B700 Mi10 UF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HP3AEU PC (Europe-Africa-Middle East) Lexan HP3AEU resin is a medium flow polycarbonate with mold release designed for medical devices and pharmaceutical applications. It is assessed with biocompatible ISO10993 (or USP Class VI) and is.. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® IFX3420Z PC (Asia Pacific) Lexan* IFX3420Z is a medium viscosity, release containing, injection moldable, polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grades meets the transm.. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® OQ4820 PC (Europe-Africa-Middle East) LEXAN OQ4820 is a high viscosity grade with a UV cut-off up to 400 nm and a greater optical purity than standard resins. Fields of application for this material are optical lenses, f.i. in sun glass.. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength at Break | <= 70.0 MPa | <= 10200 psi | ISO/R527 |
Polykemi AB POLYfill PPH GF5020 PD1 VT2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled, Heat Stabilized Information provided by Polykemi AB |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Europe-Africa-Middle East) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXD104R PC (Asia Pacific) FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXD164R PC (Europe-Africa-Middle East) Transparent/translucent medium viscosity PC for light diffusion special effects, FDA compliant and mold release containing. The color package may affect performance.This data was supplied by SABIC-I.. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | ISO 527-1/-2 |
Lanxess Pocan® B 3215 XF 901510 PBT, 10% Glass Fiber PBT, 10% glass fibers, injection molding, improved flowability, impact modified |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Asia Pacific) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | ISO 527 Type 1A |
Solvay TECHNYL® B 50 H1 PA66/6, DRY Description: TECHNYL® B 50H1 is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is av.. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp AF0029 ABS LNP* Thermocomp* AF0029 is an ABS base resin containing Glass Fiber. Characteristics of this grade are Flame Retardancy.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP AF003 ABS (Asia Pacific) LNP* Thermocomp* AF003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | ISO 527-1/-2 |
Unitika A3130HR-25 PA6, 25% Mineral Reinforced, Dry Information provided by Unitika Ltd. |
|||
Tensile Strength at Break | 70.0 - 72.0 MPa | 10200 - 10400 psi | DIN 53455 |
Zell-Metall Engineering Plastics Zellamid 1100 MO at 50% RH Improved sliding and self-lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.Color: blackApplications: For conveyor screws |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | ISO 527; DIN 53455 |
Zell-Metall Engineering Plastics Zellamid 900 (POM-C) Zellamid® 900 is the registered trademark of Zell-Metalls high molecular weight Acetal resin.Acetal (POM) is noted for its high mechanical strength, heat resistance and good antifriction .. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527-1,-2 |
Covestro Makrolon® 2652 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527-1,-2 |
Covestro Makrolon® 3152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BK-30 PA6-GB30 Information provided by EMS Grivory |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50mm/min; ISO 527 |
Teijin Panlite® GS-3410 Friction and Abrasion Resistant, Glass Fiber Reinforced Polycarbonate Resin GF 10% reinforced grade, meeting UL 94 V-2. It is compounded with fluorine powder to improve friction and abrasion resistance, maintaining excellent characteristics of polycarbonate resin.Applicatio.. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF VX99810 Super Tough Nylon Super Tough Nylon, Proprietary Filler(s), |