Polymer Property : Tensile Strength at Break = 188 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 188 MPa
27300 psi
ASTM D638
LNP Thermocomp® EF-1006 BK8-114 Polyetherimide, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Tensile Strength at Break 188 MPa
27300 psi
ISO 527-2
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA), 33% Glass Fiber
Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; ..
Tensile Strength at Break 188 MPa
27300 psi
Type I, 5 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Stat-kon EX08308C PEI (Asia Pacific)
Stat-Kon* EX08308C is a high cleanliness Polyetherimide Compound reinforced with Carbon Fiber for use in applications requiring the highest level of cleanliness. This compound is compounded using LN..
Tensile Strength at Break 188 MPa
27300 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP EF006 PEI
LNP THERMOCOMP* EF006 is a compound based on Polyetherimide resin containing 30% Glass Fiber.
Tensile Strength at Break 188 MPa
27300 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp EF008EXP PEI (Europe-Africa-Middle East)
LNP* Thermocomp* EF008EXP is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SABIC-IP ..
Tensile Strength at Break 188 MPa
27300 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF008 PA 66 (Asia Pacific)
LNP Thermocomp RF008 is a compound based on PA66 resin containing glass fiber. It is used in many applications requiring high strength over weight performance. Also known as Thermocomp RF-1008
Tensile Strength at Break 188 MPa
27300 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF008H PA 66
LNP* THERMOCOMP* RF008H is a compound based on Nylon 66 containing 40% Glass Fiber. Added feature of this grade is: Healthcare.
Tensile Strength at Break 188 MPa
27300 psi
ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF008XXZ PA 66
LNP THERMOCOMP* RF008XXZ is a compound based on Nylon 66 resin containing 40% Glass Fiber.
Tensile Strength at Break 188 MPa
27300 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RX09411H PA 66
LNP* Thermocomp* RX09411H is a compound based on Nylon 66 containing Proprietary Fillers. Characteristics are: Radiopacity and Healthcare.
Tensile Strength at Break 188 MPa
27300 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RX10405H PA 66
LNP* Thermocomp* RX10405H is a compound based on Nylon 6/6 containing Carbon Fiber. Characteristics of this grade are: Healthcare.
Tensile Strength at Break 188 MPa
27300 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP UCF22S PPA
LNP* Thermocomp* UCF22S is a compound based on Polyphthalamide resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Heat Stabilized, Electrically Conductive..
Tensile Strength at Break 188 MPa
27300 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON RX970079 PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RX970079 is a compound based on PA 66 resin containing Long Glass Fiber and PTFE. Added features include; Internally Lubricated.
Tensile Strength at Break 188 MPa
27300 psi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G25HSL NC010 is a 25% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform..
Tensile Strength at Break 188 MPa
27300 psi
ISO 527-2
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA)  (Unverified Data**)
Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade. Natural: HFZ A-1133 L NT Black: HFZ A-1133 L BK 937Information provided by Solvay Specialty Polymers.
Tensile Strength at Break 188 MPa
27300 psi
ISO 527
SABIC Innovative Plastics LNP LUBRICOMP QCP36 PA 6/10 (Asia Pacific)
LNP* Lubricomp* QCP36 is a compound based on Nylon 6/10 resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Internally Lubricated, , Electrically Conducti..
Tensile Strength at Break 188 MPa
27300 psi
ISO 527
SABIC Innovative Plastics LNP VERTON PX00700 PA 6
LNP VERTON* PX00700 is a compound based on Nylon 6 resin containing proprietary fillers. Added feature of this grade is: Structural.
Tensile Strength at Break 188 MPa
27300 psi
ISO 527
SABIC Innovative Plastics LNP VERTON PX00700 PA 6 (Asia Pacific)
LNP* Verton* PX00700 is a compound based on Nylon 6 resin containing Long Glass Fiber.