| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP THERMOCOMP |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics LNP THERMOCOMP RF008H PA 66.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
| Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
| 1.478 g/cc | 0.05340 lb/in³ | ASTM D792 | |
| Moisture Absorption | 0.600 % | 0.600 % | 50% RH, 24 hrs; ASTM D570 |
| 0.970 % | 0.970 % | 23°C / 50% RH; ISO 62 | |
| Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm <br>@Time 86400 sec |
0.0010 - 0.0030 in/in <br>@Time 24.0 hour |
ISO 294 |
| 0.0020 - 0.0040 cm/cm <br>@Time 86400 sec |
0.0020 - 0.0040 in/in <br>@Time 24.0 hour |
ASTM D955 | |
| Linear Mold Shrinkage, Transverse | 0.010 - 0.030 cm/cm <br>@Time 86400 sec |
0.010 - 0.030 in/in <br>@Time 24.0 hour |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 184 MPa | 26700 psi | Type I, 5 mm/min; ASTM D638 |
| 188 MPa | 27300 psi | 5 mm/min; ISO 527 | |
| Elongation at Break | 2.5 % | 2.5 % | Type I, 5 mm/min; ASTM D638 |
| 2.7 % | 2.7 % | 5 mm/min; ISO 527 | |
| Tensile Modulus | 12.2 GPa | 1770 ksi | 1 mm/min; ISO 527 |
| 13.3 GPa | 1930 ksi | 5 mm/min; ASTM D638 | |
| Flexural Strength | 275 MPa | 39900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 287 MPa | 41600 psi | ISO 178 | |
| Flexural Modulus | 10.41 GPa | 1510 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 12.1 GPa | 1750 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 11.37 J/cm | 21.30 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 13.0 kJ/m² | 6.19 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 74.0 kJ/m² | 35.2 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 10.0 J <br>@Temperature 23.0 °C |
7.38 ft-lb <br>@Temperature 73.4 °F |
ASTM D3763 |
| Impact Test | 3.00 J | 2.21 ft-lb | Multiaxial Impact; ISO 6603 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 25.2 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 |
| 26.8 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
14.9 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 57.6 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
32.0 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 |
| 59.2 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
32.9 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Deflection Temperature at 1.8 MPa (264 psi) | >= 240 °C | >= 464 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 252 °C <br>@Thickness 3.20 mm |
486 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 |