Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 1100-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-15 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 1100V-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100V-15 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator.. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 3101-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-15 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Izod Impact, Unnotched | 4.80 J/cm @Temperature -30.0 °C |
8.99 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics Cycoloy® C4210HF PC+ABS PC+ABS Blend with 10% Glass Reinforce. High flow, High heat resistance., Excellent balance strength/rigidity. Good impact/appearance. |
|||
Izod Impact, Unnotched | 4.80 J/cm @Thickness 3.18 mm |
8.99 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Emi-X® OC-1008 LEX Polyphenylene Sulfide, Carbon Fiber Reinforcement
(discontinued **) Features: Radio Frequency Shielding, Electromagnetic Shielding, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data .. |
|||
Izod Impact, Unnotched | 4.80 J/cm @Thickness 3.18 mm |
8.99 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® JF-1004 EM M BK905 Polyethersulfone, Milled Glass Fiber
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Izod Impact, Unnotched | 4.80 J/cm @Thickness 3.18 mm |
8.99 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Lubricomp® EFL-4034 LE BK8-065 Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued ** Features: Low Extractables, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g.. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2100 PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2100F PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 listing. WRAS certification in recognized col.. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2100F PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 listing, WRAS certification in recognized colors.. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2210R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2212EPR PEI (Asia Pacific) 20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DEL13EXC PC (Asia Pacific) LNP* STAT-KON* DEL13EXC is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Unnotched | 4.80 J/cm @Thickness 3.18 mm |
8.99 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® R-4-220BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur.. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 4521 PBT (Asia Pacific) 19.5% glass reinforced PBT. High flow, flame retardant. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DX04489C PC LNP STAT-KON* DX04489C is a high modulus compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Con.. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON EX01696C PEI (Asia Pacific) LNP* Stat-kon* EX01696C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF005 PA 66 LNP* THERMOCOMP* RF005 is a compound based on Nylon 66 resin containing 25% Glass Fiber. |
|||
Izod Impact, Unnotched | 4.80 J/cm @Temperature 23.0 °C |
8.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp WC003P Polyester Elastomer LNP* Thermocomp* WC003P is a compound based on Polyester resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A.. |
|||
Izod Impact, Unnotched | 4.80 J/cm @Temperature 23.0 °C |
8.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp KCL36 Acetal Copoly LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP KCL36 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D256 |
Adell ER-18 Homopolymer Polypropylene, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM Test |
BASF Ultramid® 8262G HS BK-102 7/13% Glass/Mineral Filled PA6 (Dry) Ultramid 8262G HS BK-102 is a heat stabilized, pigmented black, 20% glass and mineral reinforced PA6 injection molding compound resulting in a balance of engineering properties with excellent dimens.. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 753 Glass Reinforced, Flow Enhanced, PPS Alloy, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 4.80 - 5.20 J/cm @Temperature 23.0 °C |
8.99 - 9.74 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RI 548/H Rigid PVC, Antishock Injection Molding Electric antishock fittings |
|||
Izod Impact, Unnotched | 4.80 J/cm @Temperature -40.0 °C |
8.99 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Adell RR-39 Polypropylene Copolymer; 43% Glass Reinforced, High Impact Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry
(discontinued **) Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg.. |