Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.70 J/cm | 14.4 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2550® AM CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas 2550® AM CR-SX is an advanced fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications where stringent flame spread and smoke generati.. |
|||
Izod Impact, Unnotched | 7.70 J/cm | 14.4 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2550® CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas 2550® CR-SX is an advanced fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications where stringent flame spread and smoke generation .. |
|||
Izod Impact, Unnotched | 7.70 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
14.4 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PP 1373 PRE-ELEC PP 1373 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Izod Impact, Unnotched | 7.69 J/cm | 14.4 ft-lb/in | ASTM D-4812 |
PlastiComp Complet® LCF30-PA12 Nylon 12, 30% Long Carbon Fiber Content Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 12 with 30% long carbon fiber reinforcementInformation provided by PlastiComp, I.. |
|||
Izod Impact, Unnotched | 7.70 J/cm | 14.4 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high .. |
|||
Izod Impact, Unnotched | 7.70 J/cm | 14.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East) VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings. |
|||
Izod Impact, Unnotched | 7.70 J/cm @Temperature -30.0 °C |
14.4 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East) VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings. |
|||
Izod Impact, Unnotched | 7.70 J/cm | 14.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® IQ420 PBT Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Izod Impact, Unnotched | 7.70 J/cm | 14.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® IQ420 PBT (Asia Pacific) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Izod Impact, Unnotched | 7.70 J/cm | 14.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® IQ420 PBT (Europe-Africa-Middle East) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Izod Impact, Unnotched | 7.70 J/cm | 14.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® IQ420HP PBT (Asia Pacific) Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Izod Impact, Unnotched | 7.68 J/cm | 14.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP LC00APXQ PEEK LNP* THERMOCOMP* LC00APXQ is a compound based on Polyetheretherketone resin containing 50% Carbon Fiber. Added features of this material include: Exceptional Processing, Electrically Conductive. |
|||
Izod Impact, Unnotched | 7.71 J/cm | 14.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP LX03447 PEEK LNP* THERMOCOMP* LX03447 is a compound based on Polyetheretherketone containing Proprietary Filler(s). |
|||
Izod Impact, Unnotched | 7.68 J/cm | 14.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP VERTON MV006S PP LNP* VERTON* MV006S is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this material include: Chemically Coupled, Structural. |
|||
Izod Impact, Unnotched | 7.68 J/cm | 14.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP VERTON MV006S PP (Asia Pacific) LNP VERTON* MV006S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Izod Impact, Unnotched | 7.68 J/cm | 14.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP VERTON MV006S PP (Europe-Africa-Middle East) LNP VERTON* MV006S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Izod Impact, Unnotched | 7.68 J/cm @Temperature -30.0 °C |
14.4 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA High flow PPO+PA. Power distribution box applications. |
|||
Izod Impact, Unnotched | 7.68 J/cm @Temperature -30.0 °C |
14.4 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA (Asia Pacific) High flow PPO+PA. Power distribution box applications. |
|||
Izod Impact, Unnotched | 7.70 J/cm | 14.4 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Izod Impact, Unnotched | 7.70 J/cm | 14.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® IQ420HP PBT Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Izod Impact, Unnotched | 7.70 J/cm | 14.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® IQ420HP PBT (Europe-Africa-Middle East) Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Izod Impact, Unnotched | 7.70 J/cm | 14.4 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comshield® 120 Copolymer Polypropylene, Electrically Conductive - Carbon Black Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 7.70 J/cm | 14.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP VERTON MV006BS PP LNP* VERTON* MV006BS is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this grade include: Heat Stabilized, Burst Pressure, Structural, Chemically Coupl.. |