Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact Unnotched = 8.57 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 CU90 Nylon 6.6 for injection molding, 90% copper filled
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 1.80 J/cm² - NB

@Temperature -40.0 - -20.0 °C
8.57 ft-lb/in² - NB

@Temperature -40.0 - -4.00 °F
Average value: 7.38 J/cm² Grade Count:8
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Charpy Impact Unnotched 1.80 J/cm² - NB
8.57 ft-lb/in² - NB
Average value: 6.85 J/cm² Grade Count:16
Overview of materials for Nylon 66, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu..
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1200-7116 ABS, with carbon fiber
Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Information provided by Lehmann & Voss & Co.KG
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1301-7294/BL PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
ISO 179/1eU
Lucite International Diakon® MG100 Acrylic Bead Polymer, High Transparency
PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte..
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1105-7583 PEEK, with glass fiber and PTFE, improved wear resistance
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Chemical and hydroly..
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 1700-1401 PPO, with carbon fiber and glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 80-8030 Polyacetal-copolymer, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
ISO 179
Vyncolit X640 Resole Phenolic
Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties.USES: Information provided by Vyncolit, a Sumitomo Bak Group
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
ISO 179
Chi Mei Kibisan® PN-106 L150 SAN
High Clarity
Charpy Impact Unnotched 1.80 J/cm²

@Temperature -30.0 °C
8.57 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 1102 H Polypropylene
Grade with high processing stability for packaging tapes, film tape, fibrillated film, monofilaments, thermoformed and blow molded parts.Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 1.80 - 3.00 J/cm²
8.57 - 14.3 ft-lb/in²
ISO 179
Bulk Molding Compounds tetra-DUR F 4401 Bulk Molding Compound
UL-licensed, general purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prot..
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
Conditioned; ISO 179/IeU
Addiplast Addilene PMD 50271 Flame Retardant Polypropylene
Flame retardant, high rigidityInformation provided by Addiplast.
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
ISO179
Beijing Chemical Industry KAIFA® S-206 PPS Resin
Glass fiber reinforced and mineral filledInformation provided by Beijing Chemical Industry Research Institute (Group)
Charpy Impact Unnotched 1.80 - 9.50 J/cm²
8.57 - 45.2 ft-lb/in²
Average value: 4.38 J/cm² Grade Count:4
Overview of materials for Nylon 66, 40% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in..
Charpy Impact Unnotched 1.80 - 8.50 J/cm²
8.57 - 40.5 ft-lb/in²
Average value: 4.46 J/cm² Grade Count:77
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..
Charpy Impact Unnotched 1.80 J/cm²

@Temperature -30.0 °C
8.57 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 3300 MC Polypropylene
Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 1.80 J/cm²

@Temperature 23.0 °C
8.57 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styrolution Luran® 368 R Crystal Clear Transparent 77851 SAN
Description: General-purpose grade with well-balanced properties, suitable for injection molding and extrusion. Especially for applications where highest transparency and low natural color is requir..
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
ISO 179/1eU
Lucite International Diakon® MG102 Acrylic Bead Polymer, High Transparency
PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte..
Charpy Impact Unnotched 1.80 - 2.60 J/cm²
8.57 - 12.4 ft-lb/in²
Average value: 2.00 J/cm² Grade Count:6
Overview of materials for Acrylic, Optical Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of..
Charpy Impact Unnotched 1.80 - 8.20 J/cm²

@Temperature -30.0 - -20.0 °C
8.57 - 39.0 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 5.75 J/cm² Grade Count:14
Overview of materials for Polypropylene, Long Glass Fiber 50%
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include..
Charpy Impact Unnotched >= 1.80 J/cm²
>= 8.57 ft-lb/in²
ISO 179
Bulk Molding Compounds tetra-DUR N 4203 Bulk Molding Compound
Highest dimensional stability under temp. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipat..