Mechanical Properties Metric English Comments
Charpy Impact Unnotched 1.30 - 1.50 J/cm²
6.19 - 7.14 ft-lb/in²
ISO 11542-2
Okulen® 1000 - REG PE Colored
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Charpy Impact Unnotched 1.30 - 1.60 J/cm²
6.19 - 7.61 ft-lb/in²
Injection; ISO 179/1eU
Raschig Group 2557 AMC Polyester
Glass fiber reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, exceptional processability with short cycle time and low ..
Charpy Impact Unnotched 1.30 - 8.00 J/cm²

@Temperature -40.0 - -30.0 °C
6.19 - 38.1 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 4.15 J/cm² Grade Count:6
Overview of materials for Polyphthalamide (PPA), Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of ..
Charpy Impact Unnotched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179-1
Polycasa SAN
QUINN SAN sheets are characterized by good optical properties and a brilliant surface. The QUINN SAN range contains sheets that are easy to handle, to vacuum form, and show a very good dimensional s..
Charpy Impact Unnotched 1.30 - 5.50 J/cm²
6.19 - 26.2 ft-lb/in²
Average value: 3.10 J/cm² Grade Count:19
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
Charpy Impact Unnotched 1.30 - 2.50 J/cm²
6.19 - 11.9 ft-lb/in²
Average value: 1.65 J/cm² Grade Count:15
Overview of materials for Cyclo Olefin Polymer
This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria..
Charpy Impact Unnotched 1.30 J/cm² - NB
6.19 ft-lb/in² - NB
Average value: 5.12 J/cm² Grade Count:16
Overview of materials for Styrene-Butadiene Copolymer, SBC
This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values ..
Charpy Impact Unnotched 1.30 J/cm² - NB

@Temperature -40.0 - 30.0 °C
6.19 ft-lb/in² - NB

@Temperature -40.0 - 86.0 °F
Average value: 5.41 J/cm² Grade Count:27
Overview of materials for Nylon 6, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ..
Charpy Impact Unnotched 1.30 - 999.9 J/cm²

@Temperature -40.0 - 30.0 °C
6.19 - 4759 ft-lb/in²

@Temperature -40.0 - 86.0 °F
Average value: 3.55 J/cm² Grade Count:49
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
Charpy Impact Unnotched 1.30 J/cm² - NB
6.19 ft-lb/in² - NB
Average value: 8.32 J/cm² Grade Count:79
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
Charpy Impact Unnotched 1.30 J/cm²
6.19 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 1301-8524 PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Charpy Impact Unnotched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179/1eU
Polyplastics TOPAS® 5013 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade)
This grade is characterized by its high flowability and superior optical properties. It is suitable for optical components such as lenses and light guide panels where high molded precision is indisp..
Charpy Impact Unnotched 1.30 J/cm²

@Temperature 23.0 °C
6.19 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Topas Advanced Polymers TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC)
TOPAS® 5013L-10 is a high flow, internally lubricated injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, che..
Charpy Impact Unnotched 1.30 J/cm²

@Temperature 23.0 °C
6.19 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Topas Advanced Polymers TOPAS® 5013S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 5013S-04 is a high flow injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high ..
Charpy Impact Unnotched 1.30 J/cm²
6.19 ft-lb/in²
dry; ISO 179
Ter Hell Plastic K-Resin KRE 9902 Butadiene-Styrene Copolymer
Description: Butadiene-Styrene Copolymer Compound, good transparency with impact strength and stiffness well-balanced.Application: For all kinds of injection molded parts.Information provided by T..
Charpy Impact Unnotched 1.30 - 1.50 J/cm²
6.19 - 7.14 ft-lb/in²
ISO 179
Vyncolit 2950 W Novolac Phenolic
Mineral and glass fiber filled phenolic molding compound with a very high strain to failure in flexure. UL listed.USES: Armature insulation.Information provided by Vyncolit, a Sumitomo Bak Group
Charpy Impact Unnotched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179
Chi Mei Kibiton® PB-5925 SBC
Transparency, high stiffness, injection grade
Charpy Impact Unnotched 1.30 J/cm²

@Temperature -30.0 °C
6.19 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 1040 RC Polypropylene, Injection Molding Grade
Injection moldingsData was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 1.30 J/cm²

@Temperature -30.0 °C
6.19 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 1100 UC Polypropylene, Injection Molding Grade
Injection molded partsData was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 1.30 J/cm²

@Temperature -30.0 °C
6.19 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 1101 R Polypropylene
Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 1.30 J/cm²

@Temperature -30.0 °C
6.19 ft-lb/in²

@Temperature -22.0 °F
BASF Procom® T20H S63 Polypropylene
Car heater casings.Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 1.30 - 1.70 J/cm²
6.19 - 8.09 ft-lb/in²
Injection; ISO 179/1eU
Raschig Group DECAL® 152CL Phenolic
Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet..
Charpy Impact Unnotched 1.30 J/cm²

@Temperature -30.0 °C
6.19 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 1148 RC Polypropylene
Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 1.30 - 4.00 J/cm²
6.19 - 19.0 ft-lb/in²
Average value: 2.85 J/cm² Grade Count:13
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Copyright © lookpolymers.com All Rights Reserved