| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact Unnotched | 2.50 - 999.9 J/cm² @Temperature -30.0 - -20.0 °C |
11.9 - 4759 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 8.16 J/cm² Grade Count:22 |
| Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
| Charpy Impact Unnotched | 1.20 - 999.9 J/cm² @Temperature -40.0 - -20.0 °C |
5.71 - 4759 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 4.71 J/cm² Grade Count:44 |
| Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
| Charpy Impact Unnotched | 9.00 - 999.9 J/cm² @Temperature -30.0 - -30.0 °C |
42.8 - 4759 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 18.8 J/cm² Grade Count:28 |
| Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
| Charpy Impact Unnotched | 0.600 - 999.9 J/cm² @Temperature -30.0 - -30.0 °C |
2.86 - 4759 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.813 J/cm² Grade Count:19 |
| Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |
|||
| Charpy Impact Unnotched | 999.9 - 999.9 J/cm² @Temperature -60.0 - -30.0 °C |
4759 - 4759 ft-lb/in² @Temperature -76.0 - -22.0 °F |
Grade Count:6 |
| Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
| Charpy Impact Unnotched | 999.9 - 999.9 J/cm² @Temperature -60.0 - -30.0 °C |
4759 - 4759 ft-lb/in² @Temperature -76.0 - -22.0 °F |
Grade Count:20 |
| Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
| Charpy Impact Unnotched | 0.800 - 999.9 J/cm² @Temperature -30.0 - -20.0 °C |
3.81 - 4759 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.800 J/cm² Grade Count:2 |
| Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
| Charpy Impact Unnotched | 999.9 - 999.9 J/cm² @Temperature -20.0 - -20.0 °C |
4759 - 4759 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Grade Count:1 |
| Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
| Charpy Impact Unnotched | 999.9 - 999.9 J/cm² @Temperature -30.0 - -30.0 °C |
4759 - 4759 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Grade Count:7 |
| Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
| Charpy Impact Unnotched | 1.40 - 999.9 J/cm² @Temperature -40.0 - -20.0 °C |
6.66 - 4759 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 1.40 J/cm² Grade Count:3 |
| Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a.. |
|||
| Charpy Impact Unnotched | 1.10 - 999.9 J/cm² @Temperature -40.0 - -20.0 °C |
5.24 - 4759 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 2.83 J/cm² Grade Count:25 |
| Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
| Charpy Impact Unnotched | 2.90 - 999.9 J/cm² @Temperature -20.0 - -20.0 °C |
13.8 - 4759 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 7.04 J/cm² Grade Count:18 |
| Overview of materials for Polypropylene with 20% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are.. |
|||
| Charpy Impact Unnotched | 2.00 - 999.9 J/cm² @Temperature -30.0 - -30.0 °C |
9.52 - 4759 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 3.94 J/cm² Grade Count:7 |
| Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |
|||
| Charpy Impact Unnotched | 1.40 - 999.9 J/cm² @Temperature -40.0 - 30.0 °C |
6.66 - 4759 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 8.05 J/cm² Grade Count:68 |
| Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
| Charpy Impact Unnotched | 1.30 - 999.9 J/cm² @Temperature -40.0 - 30.0 °C |
6.19 - 4759 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 3.55 J/cm² Grade Count:49 |
| Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
| Charpy Impact Unnotched | 3.00 - 999.9 J/cm² @Temperature -40.0 - 30.0 °C |
14.3 - 4759 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 7.50 J/cm² Grade Count:91 |
| Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
| Charpy Impact Unnotched | 4.50 - 999.9 J/cm² @Temperature -30.0 - 30.0 °C |
21.4 - 4759 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 9.28 J/cm² Grade Count:42 |
| Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
| Charpy Impact Unnotched | 0.850 - 999.9 J/cm² @Temperature -30.0 - -30.0 °C |
4.05 - 4759 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.850 J/cm² Grade Count:3 |
| Overview of materials for Nylon 11, Cable Sheathing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Cable Sheathing Grade". Each property range of values reported is minimum and maximum values o.. |
|||
| Charpy Impact Unnotched | 5.00 - 999.9 J/cm² @Temperature -30.0 - -20.0 °C |
23.8 - 4759 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 9.26 J/cm² Grade Count:23 |
| Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
| Charpy Impact Unnotched | 5.50 - 999.9 J/cm² @Temperature -30.0 - -30.0 °C |
26.2 - 4759 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 5.50 J/cm² Grade Count:8 |
| Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
| Charpy Impact Unnotched | 27.0 - 999.9 J/cm² @Temperature -30.0 - -30.0 °C |
128 - 4759 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 27.0 J/cm² Grade Count:3 |
| Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
| Charpy Impact Unnotched | 10.0 - 999.9 J/cm² @Temperature -30.0 - -30.0 °C |
47.6 - 4759 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 10.0 J/cm² Grade Count:5 |
| Overview of materials for Nylon 66, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
| Charpy Impact Unnotched | 999.9 - 999.9 J/cm² @Temperature -30.0 - -30.0 °C |
4759 - 4759 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Grade Count:2 |
| Overview of materials for Nylon 11, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
| Charpy Impact Unnotched | 0.650 - 999.9 J/cm² @Temperature -40.0 - -20.0 °C |
3.09 - 4759 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 3.16 J/cm² Grade Count:26 |
| Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
| Charpy Impact Unnotched | 2.00 - 999.9 J/cm² @Temperature -20.0 - -20.0 °C |
9.52 - 4759 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 3.42 J/cm² Grade Count:14 |
| Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |
|||
| Charpy Impact Unnotched | 1.40 - 999.9 J/cm² @Temperature -30.0 - -30.0 °C |
6.66 - 4759 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 4.32 J/cm² Grade Count:113 |
| Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
| Charpy Impact Unnotched | 1.50 - 999.9 J/cm² @Temperature -20.0 - -20.0 °C |
7.14 - 4759 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 5.63 J/cm² Grade Count:9 |
| Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |
|||
| Charpy Impact Unnotched | 0.500 - 999.9 J/cm² @Temperature -20.0 - -20.0 °C |
2.38 - 4759 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 0.500 J/cm² Grade Count:7 |
| Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |
|||
| Charpy Impact Unnotched | 0.500 - 999.9 J/cm² @Thickness 102 - 102 mm |
2.38 - 4759 ft-lb/in² @Thickness 4.00 - 4.00 in |
Average value: 0.500 J/cm² Grade Count:7 |
| Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |
|||
| Charpy Impact Unnotched | 2.20 - 999.9 J/cm² @Temperature -30.0 - 30.0 °C |
10.5 - 4759 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 3.22 J/cm² Grade Count:6 |
| Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |
|||