Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 10.0 J/cm² @Temperature -30.0 °C |
47.6 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® BFL2015 PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Charpy Impact Unnotched | >= 10.0 J/cm² | >= 47.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® EXRL1061 PC (Asia Pacific) Transparent Polycarbonate in natural color. Excellent processability, super high flow. |
|||
Charpy Impact Unnotched | 10.0 J/cm² | 47.6 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 7-0755 Polyamide 610, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.Improved friction and wear behaviou.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² | 47.6 ft-lb/in² | |
Ineos ABS Lustran® H702 Medium heat resistance, increased flow. ,Property data per ISO test methods. |
|||
Charpy Impact Unnotched | 10.0 J/cm² | 47.6 ft-lb/in² | |
Ineos ABS Lustran® H802 High heat resistance, increased flow.,Property data per ISO test methods. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Grupo Repol Dinalon® A1S25 G50 PA66 50% Glass Fiber Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Charpy Impact Unnotched | 10.0 J/cm² | 47.6 ft-lb/in² | |
LATI Latamid 12 G/50 PA 12, 50% Glass Fiber Reinforced Polyamide 12 (PA12) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Charpy Impact Unnotched | 10.0 J/cm² | 47.6 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 218G1 V30 Black 34N PA66, 30% glass fiber, Conditioned Description: Polyamide 66, reinforced with 30% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. For 7.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² | 47.6 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® C 216 V30 PA6, 30% glass fiber, DRY Description: Polyamide PA6, reinforced with 30 % of glass fiber, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: It has good mechanical properties, it is used.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² | 47.6 ft-lb/in² | |
Covestro Makrolon® 9415(Z) Polycarbonate Medium viscosity, flame retardant extrusion and injection molding grade with 10% standard glass fibers and easy mold release agent.Information provided by Bayer.As of 1 September 2015, Bayer Materia.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² | 47.6 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BS EC PA6 Product description: Grilon BS 23 is an unreinforced, low viscosity and fine crystalline PA 6 injection molding grade. Grilon BS 23 has the following important properties: Good flow behaviorEasy pro.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² | 47.6 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GM-4H PA*-MD40 Product description: Grivory GM-4H natural is a 40 % mineral reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide. G.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² | 47.6 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® TW241F10 (COND) Nylon 46 50% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact Unnotched | 10.0 J/cm² | 47.6 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GVL-5H black 9839 PA*-GF50 Product description: Grivory GVL-5H black 9839 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² | 47.6 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSG-50 FA PA666-GF50 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 10.0 J/cm² | 47.6 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-50/4 black 9833 PA666-GF50 Product description: Grilon TSGL-50/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 black is characterized by the following key-p.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² | 47.6 ft-lb/in² | 50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 74G33J NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Polyamide 66 + Polyamide 6 Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | >= 10.0 J/cm² | >= 47.6 ft-lb/in² | Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide AST03 PA66, Impact Modified, Injection Molded AST03 is an Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Charpy Impact Unnotched | 10.0 J/cm² | 47.6 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BK-30 PA6-GB30 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Conditioned) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature -30.0 °C |
47.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultramid® B3K PA6 (Dry) Ultramid B 3K is an easy flowing, stabilized for fast processing, grade of nylon 6. |
|||
Charpy Impact Unnotched | >= 10.0 J/cm² | >= 47.6 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® MN-401 PA6 Resin Good toughnessInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Charpy Impact Unnotched | 10.0 J/cm² | 47.6 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TS V0 PA666 Product description: Grilon TS V0 is an unreinforced, normal viscosity, self-extinguishing Polyamid 66 + Polyamide 6 injection molding grade. Grilon TS V0 is halogen free and free of red phosphorous.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature -30.0 °C |
47.6 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa SINKRAL G323 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-16-20 General purpose injection moulding grade. Main properties are: good impact resistance high flow e.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² | 47.6 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss PLASLUBE NY-1/SI/2/NT Polyamide 66, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Information provided by Lehmann .. |