Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.500 - 0.700 J/cm² @Temperature 23.0 °C |
2.38 - 3.33 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eU |
Raschig Group 6552 DAIP Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Charpy Impact Unnotched | 0.500 - 0.700 J/cm² | 2.38 - 3.33 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group DECAL® 666/8/2B Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe.. |
|||
Charpy Impact Unnotched | 0.500 - 1.00 J/cm² | 2.38 - 4.76 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group RALUPOL® 4802 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Charpy Impact Unnotched | >= 0.500 J/cm² | >= 2.38 ft-lb/in² | 1eU; ISO 179 |
Perstorp Compounds AMITEC 751 Melamine Perstorp dinnerware compression and injection grade. Porcelain like properties suitable for household applications.Information provided by Perstorp Compounds Inc. |
|||
Charpy Impact Unnotched | 0.500 J/cm² - NB | 2.38 ft-lb/in² - NB | Average value: 8.45 J/cm² Grade Count:67 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Charpy Impact Unnotched | 0.500 - 1.00 J/cm² | 2.38 - 4.76 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group RALUPOL® 802 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength, good heat resistance. This product meets the allowed up.. |
|||
Charpy Impact Unnotched | 0.500 - 1.00 J/cm² | 2.38 - 4.76 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group RALUPOL® 804 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m.. |
|||
Charpy Impact Unnotched | 0.500 - 1.00 J/cm² @Temperature 23.0 °C |
2.38 - 4.76 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eU |
Raschig Group RALUPOL® 8601 UP Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic moulding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical stren.. |
|||
Charpy Impact Unnotched | 0.500 J/cm² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
SABIC Innovative Plastics Lexan® HP1HF PC (Asia Pacific) Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Charpy Impact Unnotched | 0.500 J/cm² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 38110 Phenolic Formaldehyde Resin, High Surface Quality
(discontinued **) Phenolic molding compound, mainly organically filled.Application areas: Devices for the electrical installation, pan handles, knobs, mainly for compression molding.Information provided by Bak AGBak .. |
|||
Charpy Impact Unnotched | 0.500 - 4.30 J/cm² | 2.38 - 20.5 ft-lb/in² | Average value: 1.94 J/cm² Grade Count:28 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% .. |
|||
Charpy Impact Unnotched | 0.500 J/cm² - NB | 2.38 ft-lb/in² - NB | Average value: 6.83 J/cm² Grade Count:271 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Charpy Impact Unnotched | 0.500 J/cm² | 2.38 ft-lb/in² | |
LATI Larton CE/60 PPS, 60% Mineral Reinforced Polyphenylene Sulfide (PPS) based compound. Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; .. |
|||
Charpy Impact Unnotched | 0.500 J/cm² | 2.38 ft-lb/in² | |
LATI Latene® AG7H K/30 PP Homopolymer, 30% Carbon Fiber Reinforced, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Carbon fiber. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort.. |
|||
Charpy Impact Unnotched | 0.500 J/cm² | 2.38 ft-lb/in² | |
LATI Laticonther 52/11 CP1/600 F3 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Potentially suitable for food/medical contact application.Availability: Africa & Middle East; Asia Pacific.. |
|||
Charpy Impact Unnotched | 0.500 J/cm² | 2.38 ft-lb/in² | |
LATI Laticonther 52/35 CP1/45 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Charpy Impact Unnotched | 0.500 J/cm² | 2.38 ft-lb/in² | |
LATI Laticonther 82 CP1/800 PA12 High thermal conductivity product based on Polyamide 12 (PA12). Special fillerAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Charpy Impact Unnotched | 0.500 J/cm² | 2.38 ft-lb/in² | |
LATI Latilub 80-10T Y/15 PPS, 15% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Charpy Impact Unnotched | 0.500 J/cm² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
|
Styrolution NOVODUR® P2H-AT ABS, Injection Grade Standard injection molding grade, easy flow, high gloss, hard, antistatic.Applications: Telephones, household goods, video and audio industry, office equipment. |
|||
Charpy Impact Unnotched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179 |
Styrolution PS 156F GPPS Styrolution PS 156F is a general purpose polystyrene grade with excellent flow properties, high heat resistance and is zinc stearate free.Free of internal lubricantsHigh heat resistanceExcellent flo.. |
|||
Charpy Impact Unnotched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179 |
Styrolution PS 416N HIPS Styrolution PS 416N is medium impact polystyrene with very good flow properties. It has a high rigidity whilst displaying a very good surface gloss.Very good flow propertiesHigh rigidityVery good su.. |
|||
Charpy Impact Unnotched | 0.500 J/cm² | 2.38 ft-lb/in² | IS0179-1:2000 |
Zhejiang Juner PP6-1JE PP For Automotive Parts Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Charpy Impact Unnotched | 0.500 J/cm² @Temperature -20.0 °C |
2.38 ft-lb/in² @Temperature -4.00 °F |
Notched/Unnotched not specified; ASTM DIN53453 |
Total PPC 4824WZ Polypropylene, Impact Copolymer ATOFINA 4824WZ is a nucleated impact copolymer. 4824WZ is characterized by improved stiffness and impact resistance, as well as low shrinkage and low warpage. It has been formulated for excellent .. |
|||
Charpy Impact Unnotched | 0.500 - 1.00 J/cm² | 2.38 - 4.76 ft-lb/in² | ISO 179 |
Bulk Molding Compounds tetra-DUR F 4001 Bulk Molding Compound UL-Licensed, Abrasion resistance, free of fiber glass.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipati.. |
|||
Charpy Impact Unnotched | 0.500 - 1.00 J/cm² | 2.38 - 4.76 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc.. |
|||
Charpy Impact Unnotched | 0.500 J/cm² | 2.38 ft-lb/in² | |
LATI Latimass 37 B01-01 D025 Bio-Polymer Specific density compound based on Bio-Polymer (PLA, PHB, ...). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Charpy Impact Unnotched | 0.500 - 1000 J/cm² | 2.38 - 4760 ft-lb/in² | Average value: 4.95 J/cm² Grade Count:70 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |
|||
Charpy Impact Unnotched | 0.500 J/cm² - NB @Temperature -40.0 - -20.0 °C |
2.38 ft-lb/in² - NB @Temperature -40.0 - -4.00 °F |
Average value: 4.14 J/cm² Grade Count:56 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |