Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 3.40 J/cm² | 16.2 ft-lb/in² | ISO 179/1eU |
Nilit FRIANYL A63 HH-FK 1020 Nylon 6.6 for injection molding, 10% glass fiber and 20% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.40 J/cm² | 16.2 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 W-GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.40 J/cm² @Temperature 23.0 °C |
16.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
PolyOne Bergadur™ PB400 G30 H UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 3.40 J/cm² | 16.2 ft-lb/in² | ISO 179 |
PolyOne Bergamid™ A70 G5 T Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 3.40 J/cm² | 16.2 ft-lb/in² | ISO 179 |
PolyOne Edgetek® QT020GFS/000 FR NATURAL - OBSOLETE Syndiotactic Polystyrene (SPS) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 3.40 J/cm² | 16.2 ft-lb/in² | ISO 179 |
PolyOne Edgetek® QT-30GF/000 Natural Syndiotactic Polystyrene (SPS) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 3.40 J/cm² | 16.2 ft-lb/in² | DIN 53453 |
Nilit RECONYL A GV30 Recycled nylon 6.6 for injection molding, 30% glass fiber reinforced Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.40 J/cm² - NB @Temperature -40.0 - 30.0 °C |
16.2 ft-lb/in² - NB @Temperature -40.0 - 86.0 °F |
Average value: 7.47 J/cm² Grade Count:193 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Charpy Impact Unnotched | 3.40 J/cm² - NB | 16.2 ft-lb/in² - NB | Average value: 4.95 J/cm² Grade Count:6 |
Overview of materials for Nylon 12, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr.. |
|||
Charpy Impact Unnotched | 3.40 J/cm² - NB @Temperature -30.0 - 30.0 °C |
16.2 ft-lb/in² - NB @Temperature -22.0 - 86.0 °F |
Average value: 5.70 J/cm² Grade Count:5 |
Overview of materials for Nylon 12, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr.. |
|||
Charpy Impact Unnotched | 3.40 J/cm² | 16.2 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105-7852 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Charpy Impact Unnotched | 3.40 J/cm² | 16.2 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105-8161 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Charpy Impact Unnotched | 3.40 J/cm² @Temperature -30.0 °C |
16.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 80-7919 Polyacetal-copolymer, with PTFE, easy flowing Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Charpy Impact Unnotched | 3.40 J/cm² | 16.2 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica.. |
|||
Charpy Impact Unnotched | 3.40 J/cm² | 16.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL GFN1 PPE+PS PPE+PS blend. 10% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui.. |
|||
Charpy Impact Unnotched | 3.40 J/cm² | 16.2 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie.. |
|||
Charpy Impact Unnotched | 3.40 J/cm² | 16.2 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105-7096 PEEK, with carbon fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Charpy Impact Unnotched | 3.40 J/cm² | 16.2 ft-lb/in² | ISO 179/1eU |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically .. |