Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 KF20 Nylon 6 for injection molding, 20% short glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.20 - 7.00 J/cm² | 10.5 - 33.3 ft-lb/in² | Average value: 5.51 J/cm² Grade Count:17 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² @Temperature -40.0 °C |
10.5 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 CV-CU 0550 Nylon 6.6 for injection molding, 5% carbon fiber reinforced, 50% copper filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 KV40 Nylon 6.6 for injection molding, 40% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.20 J/cm² - NB @Temperature -30.0 - -20.0 °C |
10.5 ft-lb/in² - NB @Temperature -22.0 - -4.00 °F |
Average value: 2.85 J/cm² Grade Count:56 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Charpy Impact Unnotched | 2.20 - 3.00 J/cm² @Temperature -30.0 - 30.0 °C |
10.5 - 14.3 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 2.52 J/cm² Grade Count:6 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Charpy Impact Unnotched | 2.20 - 9.50 J/cm² | 10.5 - 45.2 ft-lb/in² | Average value: 5.15 J/cm² Grade Count:32 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Charpy Impact Unnotched | 2.20 - 9.00 J/cm² @Temperature -40.0 - -30.0 °C |
10.5 - 42.8 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 4.59 J/cm² Grade Count:16 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1105-7760 PEEK, with carbon fiber, PTFE, lubricant modified, high viscosity Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1700-8126 PPO, with glass spheres and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance r.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1-8490 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.High dimensionally stab.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 20-8112 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 20-8286 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eU |
Lucite International Diakon® Frost 952 70 Acrylic Polymer Information provided by Lucite International |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179 |
GEHR Plastics PP-30GF Polypropylene, 30% Glass Fiber Polypropylene shows a high mechanical strength and a tensile strength, but a low notched impact strength. PP resists stress cracking and it is easy to weld. At minus temperatures it can get brittle... |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics LNP STAT-KON EX03319C PEI (Asia Pacific) LNP* Stat-Kon* EX03319C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | IS0179-1:2000 |
Zhejiang Juner PA-A7-1 Flame-Retardant & Glass Reinforced, Environmental PA66 Applications: Electric Cabinet BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | Conditioned; ISO 179/IeU |
Addiplast Addilene H 490 M10F Flame Retardant Polypropylene, 10% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eU |
Polyplastic Armlen® PP MD 40-4HS-901 Polypropylene, 40% Mineral Filled Heat stabilizedInformation provided by PolyPlastic Group. |
|||
Charpy Impact Unnotched | 2.20 - 3.50 J/cm² @Temperature -40.0 - -30.0 °C |
10.5 - 16.7 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 2.85 J/cm² Grade Count:2 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eU |
Lucite International Diakon® ST15G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed by in.. |
|||
Charpy Impact Unnotched | 2.20 - 5.00 J/cm² | 10.5 - 23.8 ft-lb/in² | Average value: 3.55 J/cm² Grade Count:15 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |
|||
Charpy Impact Unnotched | 2.20 - 999.9 J/cm² @Temperature -30.0 - 30.0 °C |
10.5 - 4759 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 3.22 J/cm² Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |