| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179 |
|
PolyOne OnForce™ LFT SF-40LCF/000 Black Polyphenylene Sulfide (PPS)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
|
|||
| Charpy Impact Unnotched |
2.20
J/cm² <br>@Temperature -40.0 °C
|
10.5
ft-lb/in² <br>@Temperature -40.0 °F
|
DIN 53453 |
|
Nilit FRIANYL A63 SG40 Nylon 6.6 for injection molding, 40% mineral filled
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Charpy Impact Unnotched | 2.20 - 7.00 J/cm² | 10.5 - 33.3 ft-lb/in² | Average value: 5.51 J/cm² Grade Count:17 |
|
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
|
|||
| Charpy Impact Unnotched |
2.20
J/cm² - NB <br>@Temperature -30.0 - -20.0 °C
|
10.5
ft-lb/in² - NB <br>@Temperature -22.0 - -4.00 °F
|
Average value: 2.85 J/cm² Grade Count:56 |
|
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor..
|
|||
| Charpy Impact Unnotched |
2.20
-
5.50
J/cm² <br>@Temperature -30.0 - -30.0 °C
|
10.5
-
26.2
ft-lb/in² <br>@Temperature -22.0 - -22.0 °F
|
Average value: 3.64 J/cm² Grade Count:5 |
|
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
|
|||
| Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | flatwise; ISO 179 1fU |
|
Lehmann & Voss LUVOCOM® 1105-7760 PEEK, with carbon fiber, PTFE, lubricant modified, high viscosity
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
|
|||
| Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | edgewise; ISO 179 1eU |
|
Lehmann & Voss LUVOCOM® 1-8490 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.High dimensionally stab..
|
|||
| Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | edgewise; ISO 179 1eU |
|
Lehmann & Voss LUVOCOM® 19-7816 Polyamide 46, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical..
|
|||
| Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | edgewise; ISO 179 1eU |
|
Lehmann & Voss LUVOCOM® 20-8112 Polyphthalamide, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
|
|||
| Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | edgewise; ISO 179 1eU |
|
Lehmann & Voss LUVOCOM® 20-8261 Polyphthalamide, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
|
|||
| Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | edgewise; ISO 179 1eU |
|
Lehmann & Voss LUVOCOM® 20-8286 Polyphthalamide, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
|
|||
| Charpy Impact Unnotched |
2.20
J/cm² <br>@Temperature -30.0 °C
|
10.5
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179 |
|
Lehmann & Voss LUVOCOM® 50-1396 Polycarbonate, with carbon fiber, glass fiber and PTFE, electrically conducting
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
|
|||
| Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | edgewise; ISO 179 1eU |
|
Lehmann & Voss LUVOCOM® 50-8022 Polycarbonate, with carbon fiber
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me..
|
|||
| Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eU |
|
Lucite International Diakon® Frost 952 70 Acrylic Polymer
Information provided by Lucite International
|
|||
| Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eU |
|
Lucite International Diakon® Frost 952 80 Acrylic Polymer
Information provided by Lucite International
|
|||
| Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179 |
|
GEHR Plastics PP-30GF Polypropylene, 30% Glass Fiber
Polypropylene shows a high mechanical strength and a tensile strength, but a low notched impact strength. PP resists stress cracking and it is easy to weld. At minus temperatures it can get brittle...
|
|||
| Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
|
SABIC Innovative Plastics LNP STAT-KON EX03319C PEI (Asia Pacific)
LNP* Stat-Kon* EX03319C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati..
|
|||
| Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179-1 |
|
Unitika A1025GO PA6, Flame Retardant, Dry
Information provided by Unitika Ltd.
|
|||
| Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | Conditioned; ISO 179/IeU |
|
Addiplast Addilene H 490 M10F Flame Retardant Polypropylene, 10% Mineral Filled
Flame retardant, mineral filled, with halogensInformation provided by Addiplast.
|
|||
| Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | Conditioned; ISO 179/IeU |
|
Addiplast Addilene H 490 M10S Flame Retardant Polypropylene
Flame retardant, mineral filled, with halogensInformation provided by Addiplast.
|
|||
| Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | Conditioned; ISO 179/IeU |
|
Addiplast Addinyl B2H G30 Flame Retardant Nylon 6, 30% Glass Bead
Flame retardant, 30% glass bead filled, with halogensInformation provided by Addiplast.
|
|||
| Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/IeU |
|
Addiplast Addilene H 442 M30 Polypropylene Homopolymer
High heat resistance, detergent stabilizedInformation provided by Addiplast.
|
|||
| Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eU |
|
Lucite International Diakon® ST15G8 Toughened Acrylic Polymer
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed by in..
|
|||
| Charpy Impact Unnotched | 2.20 - 1000 J/cm² | 10.5 - 4760 ft-lb/in² | Average value: 4.15 J/cm² Grade Count:7 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported..
|
|||