Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Nilit FRIANYL B63 CU90 Nylon 6.6 for injection molding, 90% copper filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 KF50 Nylon 6 for injection molding, 50% short glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO 179 |
Perstorp Compounds Aminel GF Melamine Fiberglass-reinforced melamine material with high dimensional stability, excellent injection properties and high thermal stabilityInformation provided by Perstorp Compounds Inc. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | |
Polimeri Europa EDISTIR N1460 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,E,085-03 High molecular weight general purpose polystyrene with good mechanical strength. This grade is especially recomme.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | |
Polimeri Europa EDISTIR N1461 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,085-03 High molecular weight general purpose polystyrene with good mechanical strength. Well suitable for injection mold.. |
|||
Charpy Impact Unnotched | 1.50 - 10.0 J/cm² | 7.14 - 47.6 ft-lb/in² | Average value: 5.14 J/cm² Grade Count:58 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Charpy Impact Unnotched | 1.50 - 7.90 J/cm² @Temperature -30.0 - -20.0 °C |
7.14 - 37.6 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 4.28 J/cm² Grade Count:29 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Charpy Impact Unnotched | 1.50 - 1.50 J/cm² @Temperature -20.0 - -20.0 °C |
7.14 - 7.14 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 1.50 J/cm² Grade Count:1 |
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1700-7910 PPO, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 20-7687 Polyphthalamide, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | |
LATI Laril 13-V1KC PPOm, Mineral Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Mineral filler. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good therm.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1301-8060 PPS, linear, with glass fiber and PTFE, high viscosity Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Low warpage, isotropic shrinkage characteristics.Improved friction and wear be.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | |
LATI Laticonther 80 GCE/650 PPS, Glass/Mineral Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Glass fibers / Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | |
LATI Latigray 82-04 CX/90 PA 12 Radiopaque compound based on Polyamide 12 (PA12). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | |
LATI Latishield 66-10A G/15 PA66, Steel/Glass Fiber Reinforced EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO 179/1eU |
Polyplastics TOPAS® 6013 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) Due to its high transparency, low levels of eluates, superior chemical resistance, and high heat deflection temperature, this grade is suitable for products such as pharmaceutical packaging and diag.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Topas Advanced Polymers TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6015S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature 30.0 °C |
7.14 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BGM-65 X V0 PA6-(GF+MD)65 Product description: Grilon BGM-65 X V0 is a flame retardant mineral and glass fiber reinforced PA6 injection molding grade. Grilon BGM-65 X V0 has the following important properties: Halogen and ph.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO 179/IeU |
Addiplast Addinyl B2H G30 Flame Retardant Nylon 6, 30% Glass Bead Flame retardant, 30% glass bead filled, with halogensInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO 179-1eU |
Barlog Plastics KEBATER BM240 PBT, 40% mineral reinforced, food grade (PBT+X)-MD40Information provided by BARLOG plastics GmbH. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 3340 PC Polypropylene Nucleated grade for injection moldings with higher transparency.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | |
BASF Procom® D 1012 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | >= 1.50 J/cm² | >= 7.14 ft-lb/in² | ISO 179 |
Bulk Molding Compounds tetra-DUR N 4111 Bulk Molding Compound Smooth, high gloss surface. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
|
BASF Procom® D 1133 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1101 N Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | |
LATI Latigray 82-05 CX/90 PA 12 Radiopaque compound based on Polyamide 12 (PA12). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² - NB @Temperature -40.0 - -20.0 °C |
7.14 ft-lb/in² - NB @Temperature -40.0 - -4.00 °F |
Average value: 3.83 J/cm² Grade Count:19 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Charpy Impact Unnotched | 1.50 - 8.00 J/cm² | 7.14 - 38.1 ft-lb/in² | Average value: 5.53 J/cm² Grade Count:33 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |