Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.00 J/cm² @Temperature -20.0 °C |
9.52 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTALEN® PQ 81 T 20 Polypropylene reinforced with mineral filler, impact modified Modified PP for injection molding with the content of 20% mineral filler. General application in all industry branches. Delivered in black color.Information Provided by Plastcom spol. s r.o. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® C2100 PC+ABS (Europe-Africa-Middle East) CYCOLOY C2100 is a flame retardant blend, specifically developed to meet the stringent requirements of mains current carrying applications. CYCOLOY C2100 combinesThis data was supplied by SABIC-IP f.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -20.0 °C |
9.52 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYblend 45FS PC/ABS-blend, Flame Retardant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -20.0 °C |
9.52 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYblend C65F PC/ABS-blend Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANAMID 66 A33^E Nylon 66, Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S RV300 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Asia Pacific) High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPM1944 PC (Asia Pacific) Medium flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). .. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PP CIP6015F VTUV Polypropylene, Mineral Reinforced, Heat and UV Stabilized Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1eA |
Lanxess Durethan® BC 550 DUSXBL 900116 Nylon 6 PA 6, non-reinforced, extrusion, Blastorm, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 179-1eA |
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -20.0 °C |
9.52 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latamid 66 E21 PA 66, Impact Modified Polyamide 66 (PA66). Toughened. Good impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p... |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax BTQ50-EQ00N1 Nylon 6, Impact Modified (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eA |
Lanxess Durethan® A 30 000000 Nylon 66 PA 66, standard injection molding grade, non-reinforced, very easy release, normal solidificationApplication Examples: terminal blocks, cable clips, bobbins, gearwheels |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eA |
Lanxess Durethan® BKV 30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade with 30% glass fibers, good heat-ageing resistance |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Asia Pacific) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis RA130E-8427 Polypropylene Random Copolymer RA130E-8427 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is grey colored. Applications: domestic water, heating, relining, plumbing, and industr.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM Akulon® S223-PG8 PA66-GF40 40% Glass Reinforced, Impact Modified |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM EcoPaXX® Q-X07209 PA410-I-GF40 % Glass Reinforced, Impact Modified |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST801AHS NC010 Nylon 66
(Unverified Data**) Zytel® ST801AHS NC010 is a Super Tough, high performance polyamide 66 resin. It offers outstanding molding performance in injection molding applications.Information provided by DuPont |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM EcoPaXX® Q-X07290 PA410-I Impact Modified |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Arkema Group Pebax® 6333 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 6333 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® B3 GF 50 RM-M (3146) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, .. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® S3 GF 50 1 (3533) PA 6.10 Dry, 50% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -40.0 °C |
9.52 ft-lb/in² @Temperature -40.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® C1100 PC+ABS (Europe-Africa-Middle East) CYCOLOY C1100 is a PC+ABS blend developed to satisfy the demanding application requirements, where optimum combination is needed of superior processing efficiency, excellent ductility also at sub ze.. |