Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 GF 30 FRG 4 LW PA6, 30% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with nonhalogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°.. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 GF 35 Polyamide 6, 35% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 35% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature -20.0 °C |
5.71 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 66 GF 35 Polyamide 66, 35% Glass Fiber FeaturesChemically reinforced with 35% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 66 GF 45 PA66, 45% glass fibre FeaturesChemically reinforced with 45% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature 20.0 °C |
5.71 ft-lb/in² @Temperature 68.0 °F |
ISO 179/1eA |
Polyplastic Armamid® PA GF50-1 Nylon 6, 50% Glass Fiber High stiffnessInformation provided by PolyPlastic Group. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature -20.0 °C |
5.71 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB SCANMID 6 B12^ F50 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® S RV300 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
PolyOne Bergamid™ A70 G25 H natur TM-X Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
PolyOne Bergamid™ B70 G/GK30 TM-Y UV NC Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® K-FHG12 (Dry) 60% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® Ultraflow™ K-FG0 Nylon 6-50% Glass Reinforced (European and Asian Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Sax Polymers SAXAMID 226F5 Nylon 6.6, 25% Glass Fiber SAXAMID 226F5 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 25% glass fibers. It has high mechanical strength in combination with good flow properties.Information provid.. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM Novamid® 1010GH30 NAT PA6-GF30 30% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Stanyl® TE200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Stanyl® TW241F8 Nylon 46-40% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 77G33HS1L NC010 Nylon 612 Zytel® 77G33HS1L NC010 is a 33% glass fiber reinforced, heat stabilized polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature -40.0 °C |
5.71 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST811HS BK038 Nylon 6
(Unverified Data**) Zytel® ST811HS BK038 is a flexible, non-plasticized, black Super Tough nylon 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores an.. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Arnitel® EL630 63 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eA |
Eurotec® Tecodur® PB70 GR30 NL PBT 30% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, DAM Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when.. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultramid® HMG14 HS BK 102 60% Glass Filled PA66 (Conditioned) Description: Ultramid HMG14 HS BK-102 is a 60% glass reinforced, injection molding grade of PA66 offering high strength and stiffness. Due to inherently lower moisture absorption, Ultramid HMG14 HS .. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® B3 GF 30 RM-M (3016) PA 6 Dry, 30% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A RV400 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Noryl EN130 PPE+HIPS (Europe-Africa-Middle East) NORYL EN130 is an extrusion material with a Vicat B/120 of 140 deg C according ISO 306. NORYL EN130 is a standard extrusion grade for applications where higher temperature resistance is required. NO.. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radiflam® A RV300AE (cond.) Nylon 66-30GF PA66 flame retardant injection molding grade. 30% Glass fiber reinforced, for items with high stiffness. Natural colorInformation provided by Radici group. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® B3WG5 BK 00654 PA6 25% Glass Filled BK (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |