Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
PolyOne OnFlex™ BIO 5180D-E0014 Thermoplastic Elastomer (TPE) OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 MI LS PA66, improved strength FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH GF5020 PD1 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANCOMP PP BN140 T5 Polypropylene Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A HSK (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® S 32HS (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH GF5020 PD1 VT2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled, Heat Stabilized Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH GF8030 PB Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A CP300K (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® Ultraflow™ K-FHGM44 Nylon 6-40% Glass and Mineral Reinforced (European and Asian Grade) (Cond)
(d The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® Ultraflow™ K-FHGM44 Nylon 6-40% Glass and Mineral Reinforced (European and Asian Grade) (Dry)
(di The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-2120 20% Talc-Filled Polypropylene Block-Copolymer INNOPOL® CS 2-2120 is a 20% talc-filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-2120 is developed for producing.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-3130 NU UV-Stabilized 30% Talc-Filled Polypropylene Block-Copolymer INNOPOL® CS 2-3130 NU is an UV-stabilized 30% talc-filled polypropylene block-copolymer compound /PP-B TD30 (ISO 1043)/.INNOPOL® CS 2-3130 NU is recommended for producing injection molded prod.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-9000 MA B Polypropylene Copolymer INNOPOL® CS 2-9000 MA B is a black colored, high melt flow copolymer with antistatic additive.INNOPOL® CS 2-9000 MA B is developed for producing injection molded automotive components.All info.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 3-9120 SR5 17% Talc Filled Polypropylene Blend INNOPOL® CS 3-9120 SR5 is a 17% talc-filled compound based on blend of polypropylene block copolymer and homopolymer. This grade is available in natural and custom colored form.INNOPOL® CS 3-9.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
|
LATI Lastilac RT K/10 ABS, 10% Carbon Fiber Reinforced Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Carbon fiber. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInforma.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis BA390TF Polypropylene Copolymer BA390TF is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA390TF is recommended for foam extrusion, or thermoforming.Inform.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis BD950MO Polypropylene Copolymer BD950MO is a heterophasic copolymer. This grade is intended for compression and injection molding. The main features of this grade are good stiffness and impact resistance, very good process ability.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Unipetrol PP MONSTEN® GB 506 Polypropylene Impact Copolymer Applications include injection molding and thermoforming. Basic stabilization. Impact copolymer.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Unipetrol PP MONSTEN® MT 825 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Unipetrol PP MONSTEN® MT 950 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Total PPC 12642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 12642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 70 g/10 min and good mechanical properties.Polypropylene PPC 10641 has been developed for high s.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Daplen™ EE189AI Polypropylene TPO Compound Daplen™ EE189AI is a 15% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. .. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eA |
DSM Stanyl® TW241B3 PA46-CF15 15% Carbon Reinforced, Heat Stabilized, Lubricated |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eA |
DSM Stanyl® TW242FM10 PA46-(GF+MF)50 50% Glass/Mineral Reinforced, Heat Stabilized |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
BASF Ultraform® Z2320 003 POM Description: Is a POM, rapidly solidifying grade for applications with exceptional demands on flowability.Information provided by BASF |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, .. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® FG101L NC010 Nylon 66
(Unverified Data**) Zytel® FG101L NC010 is a lubricated polyamide 66 resin for injection molding. It has been developed for consideration into applications such as parts for the food industry.Information provided by D.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPHC T11030 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A HSK (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |