Polymer Property : Izod Impact, Notched = 0.750 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
73°F; ASTM D256
Multibase Multi-Pro® 1510 CNU White Polypropylene
Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
ASTM D256
Nylene® Mach 6 , Fast Cycle Nylon 6
Description: Nylene® Mach is a fast cycle, high speed, high flow nylon 6. Information provided by Custom Resins.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resourc..
Izod Impact, Notched >= 0.400 J/cm
>= 0.750 ft-lb/in
ASTM D256
S&E Specialty Polymers GPP1001V0M-HCO-15 PP
Description: A medium flow polypropylene compound designed for injection molded industrial battery, electrical housing or appliance applications. It affords medium impact resistance with a high lev..
Izod Impact, Notched 0.400 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.750 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Lubri-Tech™ AT-15MCF/15T Acetal-Copolymer, Carbon Fiber Reinforced, PTFE Lubricated  (discontinued **)
Description/Features:Milled Carbon Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
Reliance Industries Polypropylene - Calcium carbonate filled
Information provided by Reliance Industries
Izod Impact, Notched 0.400 J/cm

@Thickness 3.17 mm
0.750 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA4/6 0206
Availability: North AmericaForms: PelletsFeatures: High Specific Gravity and Thermally ConductiveInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
ASTM D256
Styron EMERGEâ„¢ 4701-13 Polycarbonate
EMERGEâ„¢ PC 4701-13 advanced resin is formulated with 10% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res..
Izod Impact, Notched 0.400 J/cm

@Temperature 22.8 °C
0.750 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Teknor Apex Sinelec CCB2095 Specialty Polystyrene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Electrically Conductive Forms: Pellets Processing Method: Injection MethodInformation Provided by Teknor Ape..
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
Tra-Con Tra-Bond 2112 Rigid Epoxy Staking Compound
TRA-BOND 2112 is a thixotropic epoxy system recommended for critical electronic, aerospace and industrial bonding, laminating and reinforcing applications requiring an adhesive with high-fill, non-s..
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
Tra-Con Tra-Bond 2104 Rigid Epoxy Staking Compound
TRA-BOND 2104 is a thixotropic epoxy system recommended for critical electronic, aerospace and industrial bonding, laminating and reinforcing applications requiring an adhesive with high-fill, non-s..
Izod Impact, Notched 0.400 J/cm

@Temperature 22.8 °C
0.750 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Ensinger TECATOR™ GF30 (XP142T) Polyamide-imide (PAI), 30% glass filled, compression molded
TECATOR™ is a high performance melt processable polyamideimide that maintains its excellent mechanical and wear properties in temperature environments exceeding 500°F. Stock shapes from Ensinger ..
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0334T10L Talc Reinforced
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0334T20L Talc Reinforced
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0336C40L Calcium Reinforced
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0336M40L Mica Reinforced
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0336W20L1 Wollastonite Reinforced
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0336W30L1 Wollastonite Reinforced
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0339C20L1 Calcium Reinforced
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0339G10M20CL Glass/Mineral Reinforced Coupled
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
Atom Adhesives AA-BOND 2104 Epoxy Adhesive
AA-BOND 2104 is a thixotropic epoxy system recommended for critical electronics, aerospace and industrial bonding, laminating and reinforcing applications requiring an adhesive with high-fill, non-s..
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
Atom Adhesives AA-BOND 2112 Epoxy Adhesive
AA-BOND 2112 is a thixotropic epoxy system recommended for critical electronics, aerospace and industrial bonding, laminating and reinforcing applications requiring an adhesive with high-fill, non-s..
Izod Impact, Notched >= 0.400 J/cm
>= 0.750 ft-lb/in
ASTM D256
S&E Specialty Polymers GPP1001V0M-HCO PP
Application: A polypropylene compound designed for injection molded industrial battery, electrical housing or appliance applications.  It affords medium impact resistance with a high level of flam..
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
ASTM D256
PlastxWorld Veroplas PB2009L Nylon 66
general purpose, unfilled, lubricated injection molding gradeInformation provided by PlastxWorld Inc.