A. Schulman POLYFORT™ FPP 4020 20% Mineral-Filled Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FPP 4020 20% Mineral-Filled Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DescriptionPolyfort® FPP 4020 is a 20% mineral-filled polypropylene designed for use when improved heat resistance and high stiffness is needed.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Melt Index of Compound 4.0 - 8.0 g/10 min
4.0 - 8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 MPa
4350 psi
ASTM D638
Flexural Modulus 2.00 GPa
290 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
ASTM D648