Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.180 - 2.14 J/cm | 0.337 - 4.00 ft-lb/in | Average value: 0.563 J/cm Grade Count:25 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Izod Impact, Notched | 0.107 - 2.14 J/cm | 0.200 - 4.00 ft-lb/in | Average value: 0.596 J/cm Grade Count:13 |
Overview of materials for Epoxy Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Izod Impact, Notched | 0.107 - 2.14 J/cm | 0.200 - 4.00 ft-lb/in | Average value: 0.498 J/cm Grade Count:65 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Izod Impact, Notched | 0.160 - 2.14 J/cm | 0.300 - 4.00 ft-lb/in | Average value: 1.57 J/cm Grade Count:4 |
Overview of materials for Polyphenylene Ether, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Mineral Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Notched | 0.640 - 2.14 J/cm | 1.20 - 4.00 ft-lb/in | Average value: 1.54 J/cm Grade Count:30 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Notched | 0.961 - 2.14 J/cm | 1.80 - 4.00 ft-lb/in | Average value: 1.40 J/cm Grade Count:7 |
Overview of materials for Nylon 11 + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
Mar-Bal MB2000-8 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 100 Thermoset Polyester, GP BMC 100 is a high strength, low shrink general purpose molding compound. It can be supplied in bulk or extruded in pre-weighted slugs. Due to the excellent flow and controlled reactivity, BMC 100 is.. |
|||
Izod Impact, Notched | 1.60 - 2.14 J/cm | 3.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 1403 Electrical Grade BMC 1403 is one of the most useful general-purpose electrical grade materials available on the market. Competitive against phenolic, melamine, and urea materials for electrical applications. Easy mo.. |
|||
Izod Impact, Notched | 1.60 - 2.14 J/cm | 3.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 2270 Mineral Filled, Glass Reinforced Polyester BMC 2270 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a general purpose material with medium impact strength a.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 3001H Mineral Filled Alkyd BMC 3001H molding compound is a mineral filled, glass-fiber reinforced alkyd compound suitable for compression and transfer molding. Because of its soft flow, it is also used extensively in cold spu.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 5436 Mineral Filled, Glass Reinforced Polyester BMC 5436 molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 600 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 600 molding compound is a mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a general purpose material with medium .. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 604 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 604 molding compound is a low-cost, mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose material wit.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 605L Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605L molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 901 Encapsulating Grade Molding Compound BMC 901 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, .. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 1050 Thermoset Polyester BMC 1050 is a cosmetic, appliance grade material with superior heat stability. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical applications are toaster e.. |
|||
Izod Impact, Notched | 1.60 - 2.14 J/cm | 3.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 1423 Wear Resistant, Electrical Grade BMC 1423 is a wear-resistant electrical grade material used in applications where there are moving parts. Best anti-wear properties are exhibited when used in conjunction with mating parts molded fr.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 200 Thermoset Polyester, Electrical Grade BMC 200 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, bobbins, electrical conne.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 2201 Mineral Filled Alkyd BMC 2201 molding compound is a mineral filled, glass-fiber-and nylon-floc reinforced alkyd compound suitable for compression and transfer molding. It was developed for applications requiring better .. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 2274 Mineral Filled, Glass Reinforced Polyester BMC 2274 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression transfer and stuffer injection molding. It is a general-purpose material with medium.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 610 Mineral Filled, Glass Reinforced Polyester Compound BMC 610 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is set a part form other medium impact el.. |
|||
Izod Impact, Notched | 0.214 - 2.14 J/cm | 0.400 - 4.00 ft-lb/in | Average value: 0.673 J/cm Grade Count:190 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Izod Impact, Notched | 0.518 - 2.14 J/cm | 0.970 - 4.00 ft-lb/in | Average value: 1.24 J/cm Grade Count:30 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |