Polymer Property : Izod Impact, Notched = 0.300 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.160 J/cm
<br>@Thickness 6.35 mm
0.300 ft-lb/in
<br>@Thickness 0.250 in
ASTM D-256
Plaskolite Optix® CA - 41 FDA General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Izod Impact, Notched 0.160 J/cm
<br>@Thickness 6.35 mm
0.300 ft-lb/in
<br>@Thickness 0.250 in
ASTM D-256
Plaskolite Optix® CA - 41 UVT General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Izod Impact, Notched 0.160 J/cm
<br>@Thickness 6.35 mm
0.300 ft-lb/in
<br>@Thickness 0.250 in
ASTM D-256
Plaskolite Optix® CA - 51 HF General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Izod Impact, Notched 0.160 J/cm
<br>@Thickness 6.35 mm
0.300 ft-lb/in
<br>@Thickness 0.250 in
ASTM D-256
Plaskolite Optix® CA - 71 General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
ASTM D256
Plaskolite Optix® CA-82 General Purpose Acrylic Resin
Injection Molding Grade Pellets. Highest Molecular Weight, good heat resistance. Superior mold release.
Izod Impact, Notched 0.160 J/cm
<br>@Thickness 6.35 mm
0.300 ft-lb/in
<br>@Thickness 0.250 in
ASTM D-256
Plaskolite Optix® CP - 41 HF General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Izod Impact, Notched 0.160 J/cm
<br>@Thickness 6.35 mm
0.300 ft-lb/in
<br>@Thickness 0.250 in
ASTM D-256
Plaskolite Optix® CP - 71 General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Izod Impact, Notched 0.160 J/cm
<br>@Thickness 6.35 mm
0.300 ft-lb/in
<br>@Thickness 0.250 in
ASTM D-256
Plaskolite Optix® CP - 71 LL General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Izod Impact, Notched 0.160 J/cm
<br>@Thickness 6.35 mm
0.300 ft-lb/in
<br>@Thickness 0.250 in
ASTM D-256
Plaskolite West Optix® CA - 41 FDA General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Izod Impact, Notched 0.160 J/cm
<br>@Thickness 6.35 mm
0.300 ft-lb/in
<br>@Thickness 0.250 in
ASTM D-256
Plaskolite West Optix® CA - 75 UVA General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
ASTM D256
Plaskolite West Optix® CA-86 Clear General Purpose Acrylic Resin
General purpose acrylic resin, extrusion and injection molding gradeApplications: A general-purpose acrylic resin designed for high heat application. This resin offers the highest heat resistance a..
Izod Impact, Notched 0.160 J/cm
<br>@Thickness 6.35 mm
0.300 ft-lb/in
<br>@Thickness 0.250 in
ASTM D-256
Plaskolite West Optix® CP - 71 LL General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
0.125 inch bar; ASTM D256
Network Polymers MS 200 Styrene Methyl Methacrylate Copolymer
Description: Styrene Methyl Methacrylate CopolymerInformation provided by Network Polymers Inc.
Izod Impact, Notched 0.160 J/cm
<br>@Thickness 6.35 mm
0.300 ft-lb/in
<br>@Thickness 0.250 in
ASTM D-256
Plaskolite West Optix® CA - 41 HF General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Izod Impact, Notched 0.160 - 2.14 J/cm
0.300 - 4.00 ft-lb/in
Average value: 1.57 J/cm Grade Count:4
Overview of materials for Polyphenylene Ether, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Mineral Filled". Each property range of values reported is minimum and maximum valu..
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
ASTM D256
M. Holland Company SA311 Styrene Acrylonitrile
Medium clarityGood processabilityHigh stiffnessApplications: AppliancesCosmeticsHousehold goods
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
ASTM D256
Sumitomo Bakelite North America E 3812M-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy
E 3812M-1 is a mineral and short fiberglass filled epoxy molding compound for low pressure encapsulation molding, featuring excellent dimensional stability, good thermal shock resistance, and good e..
Izod Impact, Notched 0.160 J/cm
<br>@Thickness 3.17 mm
0.300 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
PlastxWorld CEVIAN®-N 055 SAN resin
These are typical values and are not intended for specification purposes. UL approved file No. is E142893. Information provided by PlastxWorld Inc.
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
ASTM D256
A. Schulman PP 3471-01 Polypropylene High Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 3471-01 is an ultra high flow homopolymer polypropylene designed for high speed, thin wall injection molding.Information provided by A. Schulman.
Izod Impact, Notched 0.160 J/cm
<br>@Thickness 3.17 mm
0.300 ft-lb/in
<br>@Thickness 0.125 in
injection molded sample; ASTM D256
American Polymers API 390 Polystyrene
API 390 is a general purpose polystyrene produced in pellet form for injection molding. API 390 has excellent clarity and easy flow.Applications: Used in the manufacture of cosmetic containers, hou..
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
1/8 in.; ASTM D256
Chevron Phillips EA3400 Medium Flow Crystal
DescriptionChevron EA3400 is a medium flow-crystal polystyrene resin developed to blend with Styrene-Butadiene block copolymers for sheet extrusion and vacuum thermoforming. EA3400 can be used in c..
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
ASTM D256A
Braskem FF450WV Homopolymer Polypropylene
Description: Excellent Processability, Nucleated.Applications: Suggested Uses Include Fast-Cycle Injection Molding and CompoundingProcess: Injection Molding.This resin meets the requirements for ole..
Izod Impact, Notched 0.160 J/cm
<br>@Thickness 3.17 mm
0.300 ft-lb/in
<br>@Thickness 0.125 in
injection molded sample; ASTM D256
American Polymers API 392 Polystyrene
API 392 is a general purpose polystyrene produced in pellet form for injection molding. API 392 has excellent clarity and high flow.Applications: Used in the manufacture of containers, housewares, ..
Izod Impact, Notched 0.160 - 0.587 J/cm
0.300 - 1.10 ft-lb/in
Average value: 0.322 J/cm Grade Count:8
Overview of materials for Acrylic, UV Stabilized, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of..
Izod Impact, Notched 0.160 - 1.30 J/cm
0.300 - 2.44 ft-lb/in
Average value: 0.306 J/cm Grade Count:125
Overview of materials for Acrylic, Optical Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of..