Bulk Molding Compounds BMC 1403 Electrical Grade

Category Polymer , Thermoset , Polyester, TS
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC 1403 Electrical Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
BMC 1403 is one of the most useful general-purpose electrical grade materials available on the market. Competitive against phenolic, melamine, and urea materials for electrical applications. Easy molding in compression, transfer and injection processes. Stable shelf life. UL® recognized. This material was formerly known as Glastic® 1403.
Physical Properties Metric English Comments
Specific Gravity 1.91 - 1.97 g/cc
1.91 - 1.97 g/cc
Water Absorption 0.12 - 0.16 %
0.12 - 0.16 %
24 hours, 23°C
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 40 - 50
40 - 50
Tensile Strength, Ultimate 34.5 - 41.4 MPa
5000 - 6000 psi
Flexural Strength 100 - 114 MPa
14500 - 16500 psi
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Compressive Strength 145 - 159 MPa
21000 - 23000 psi
Izod Impact, Notched 1.60 - 2.14 J/cm
3.00 - 4.00 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 17.2 kV/mm
438 kV/in
Short Time
Dissipation Factor 0.026

@Frequency 60 Hz
0.026

@Frequency 60 Hz
Condition A
0.058

@Frequency 60 Hz
0.058

@Frequency 60 Hz
Condition D
0.078

@Frequency 60 Hz
0.078

@Frequency 60 Hz
Condition A
0.119

@Frequency 60 Hz
0.119

@Frequency 60 Hz
Condition D
Arc Resistance 199 sec
199 sec
Processing Properties Metric English Comments
Mold Temperature 138 - 166 °C
280 - 330 °F