Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP AI001XXH ABS LNP* Lubricomp* AI001XXH is a compound based on ABS containing 2% Silicone. Characteristics of this grade are: Healthcare and Internally Lubricated. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFL34EH PC LNP* LUBRICOMP* DFL34EH is a compound based on Polycarbonate containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Easy Molding, Healthcare, Wear Resistant. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 5% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 5% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 1.49 J/cm @Diameter 3.17 mm |
2.79 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 5410 High Impact Polystyrene High impact, Good ESCR, Good printabilityApplications: Thermoformed containers and lids, Hot and cold beverages cups, Custom sheetProperties were determined on injection molded specimens at 23°C .. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DX94375H PC (Asia Pacific) LNP* Lubricomp* DX94375H is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL TCN8222 PPE+HIPS (Asia Pacific) PPE/HIPS unfilled 80C FR-V2 |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP PFL36 PA 6 LNP* LUBRICOMP* PFL36 is a compound based on Nylon 6 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP PFL36 PA 6 (Asia Pacific) LNP* Lubricomp* PFL36 is a compound based on Nylon 6 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM D9065 PEI Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF00AS PA 66 LNP THERMOCOMP* RF00AS is a compound based on Nylon 66 resin containing 50% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP SF006 PA 12 LNP THERMOCOMP* SF006 is a compound based on Nylon 12 resin containing 30% Glass Fiber. |
|||
Izod Impact, Notched | 1.49 J/cm @Temperature -30.0 °C |
2.79 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP PPE+PP blend. High Impact, Good Heat Resistance |
|||
Izod Impact, Notched | 1.49 J/cm @Temperature -30.0 °C |
2.79 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP (Asia Pacific) PPE+PP blend. High Impact, Good Heat Resistance |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Asia Pacific) PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Europe-Africa-Middle East) PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly LNP* STAT-LOY* K3000SZ is a compound based on Acetal Copolymer resin. Added feature of this material is: AntiSstatic. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly (Asia Pacific) LNP* Stat-loy* K3000SZ is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat. |
|||
Izod Impact, Notched | 1.49 J/cm @Temperature 23.0 °C |
2.79 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp SF006S PA 12 LNP* Thermocomp* SF006S is a compound based on Nylon 12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re.. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOTUF PX06417 PA 6 LNP THERMOTUF* PX06417 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOTUF VC006 Super Tough PA 6/6 (Asia Pacific) LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon 6/6 resin containing Carbon Fiber. Added features of this material include: High Impact. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
Unitika E-RUNG60 Ultra high-rigidity PA6, Dry Ultra high-rigidityInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 1.49 J/cm @Thickness 3.17 mm |
2.79 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultraform N 2640 Z4 UNC Q600 POM Ultraform N2640 Z4 UNC Q600 is a high toughness, elastomer-modified injection molding POM grade. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 618 Nylon 6, Mineral Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.15% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Izod Impact, Notched | 1.49 J/cm @Thickness 3.18 mm |
2.79 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® SF-1006 Polyamide 12, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 5% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36E PC LNP LUBRICOMP* DFL36E is a compound based on Polycarbonate resin containing 30% Glass Fiber, 155 PTFE. Added features of this material include: Easy Molding, Internally Lubricated. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM-D256 |
Braskem HB0454HR HDPE Blow Molding Polyethylene Copolymer HB0454HR is a high-density polyethylene copolymer resin with average molecular weight produced by the Unipol® process. A bottle made with HB0454HR shows excellent processability, color, and superfi.. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 5% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |