Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers PC-1011 L Description: Natural PolycarbonateInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 101R PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. Internal mold release. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 104R PC (Asia Pacific) LEXAN 104R is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information a.. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
Polymer Resources NY66-IM2-LM Nylon, Preliminary Data Sheet, Low Flexural Modulus, High Impact (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Izod Impact, Notched | 9.08 J/cm @Temperature 22.8 °C |
17.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-GP1-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Low Flow Polycarbonate, FDA-compliant Feedstocks, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro.. |
|||
Izod Impact, Notched | 9.08 J/cm @Temperature 22.8 °C |
17.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-UV1-D Polycarbonate, UV-stabilized, Low Flow Polycarbonate, UV-stabilized, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Po.. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXD103R PC (Asia Pacific) FXD103R is a Light Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect propert.. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HPS6 PC (Asia Pacific) Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HPS6 PC (Europe-Africa-Middle East) Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LS3 PC (Asia Pacific) Automotive lens applications. Medium-high viscosity. UV-stabilized. Adhesion to coatings. Transparent colors only. |
|||
Izod Impact, Notched | 9.07 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 303 PC (Asia Pacific) Clear, high viscosity material designed to service severe environments of HID lighting.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® AD4820 PC (Asia Pacific) LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin. |
|||
Izod Impact, Notched | 9.10 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 200-6 Polycarbonate Resin Overview: CALIBREâ„¢ 200-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance.. |
|||
Izod Impact, Notched | 9.10 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256; ISO 180/4A |
Styron CALIBREâ„¢ 201-6 Polycarbonate Resin Overview: CALIBREâ„¢ 201-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance.. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ 2060 10 Polycarbonate, Sterilization Grade CALIBRE® 2060 series resins are designed for those applications which use steam or ethylene oxide for sterilization. This material has excellent retention of physical properties and optical clari.. |
|||
Izod Impact, Notched | 9.10 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 301-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet applic.. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ MEGARAD 2080 10 Polycarbonate, Gamma Radiation Resistant CALIBRE® MegaRad 2080 series resins provide end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (g.. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
Styron EMERGEâ„¢ 4310-10 Polycarbonate EMERGEâ„¢ PC 4310-10 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq.. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
Styron CALIBREâ„¢ 2061-6 Polycarbonate CALIBREâ„¢ 2061-6 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and .. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | 0.125 in; 10 mil notch; ASTM D256 |
Styron CALIBREâ„¢ 302-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Izod Impact, Notched | 9.10 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 302V-6 Polycarbonate Resin Overview: CALIBREâ„¢ 302V-6 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity (for tinted/transparent colors), and is available in both tint.. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
Teknor Apex Sinvicomp SBB 3715 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Ultra High Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation P.. |
|||
Izod Impact, Notched | 9.10 J/cm @Thickness 3.20 mm |
17.0 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Makrolon® 2605 Polycarbonate, Injection Grade Easy flowing injection molding grade with easy mold release, Makrolon grade 2658 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separat.. |
|||
Izod Impact, Notched | 9.10 J/cm @Thickness 3.20 mm |
17.0 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Makrolon® 2658 Polycarbonate, Injection Grade Easy flowing BgVV- and FDA injection molding grade with easy mold release, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Bayer M.. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
Ensinger Tecamid® ST Nylon (PA) Super Tough nylon, increased impact resistance and toughness over nylon 6/6.Information provided by Ensinger, Inc. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 527LDS-B2 Nylon 66 A high impact lubricated nylon resin containing well dispersed carbon black for maximum resistance to weathering.Data provided by the manufacturer |
|||
Izod Impact, Notched | 9.08 J/cm @Thickness 3.17 mm |
17.0 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 6680 Rigid PVC, Molding, White 476 Georgia Gulf 6680 White 476 is a weatherable, high flow injection molding compound, specially formulated for outdoor UV exposure. This compound was designed to be used in various accessory parts, s.. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 734-SP5 Nylon 6, Flexible Grade A highly flexible grade of Nylon 6 with outstanding impact.Data provided by the manufacturer |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 103R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV Stabilized for outdoor and lighting. Internal mold release... |