Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 943 PC Opaque colors, medium viscosity, superior flame retardance. UV-stabilized. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EM3110R PC (Asia Pacific) Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. Internal mold release. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 22.8 °C |
12.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted.. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 22.8 °C |
12.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-FR2-D-[color]-3 Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 22.8 °C |
12.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-FR3-D Polycarbonate, Improved Flame Retardant, High Flow Polycarbonate, Improved Flame Retardant, High FlowFeatures: • High Impact Resistance • Self Extinguishing • Low ViscosityProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D785 |
Ravago Manufacturing Americas Hylex® P10017FRMA Polycarbonate Polycarbonate, General Purpose, Flame RetardantInformation provided by Ravago. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Tristar® PC-10R-(18) 18 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LSHF PC (Europe-Africa-Middle East) Clear PolyCarbonate, High Flow, UV Stabilization, Heat Stabilization |
|||
Izod Impact, Notched | 6.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ SF M7120 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 920A PC (Asia Pacific) Low viscosity injection moldable, flame retardant PC. Exceptional surface appearance. Clear, tints and opaque colors. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 943A PC (Asia Pacific) Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HF1140 PC (Europe-Africa-Middle East) Ideal for disposables/short life cycles. Good clarity, heat resistance, property retention and dimensional stability. FDA food contact compliant in limited colors.Effective January 15th, 2007 this.. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Ravago Manufacturing Americas Hybrid S470H Acrylonitrile Butadiene Styrene + PC Alloy Available in North America Flame Retardant RoHS Compliant UL File Number: E157012 Form: Pellets Processing Method: Injection Molding Information provided by Ravago |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® ML4539 PC Polycarbonate for aircraft applications requiring FAR 25.853a compliance. Injection moldable. Opaque colors. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Lucent Polymers PC-1418 Polycarbonate, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
MRC Polymers NAXALOYâ„¢ 770-BK272 ABS + PC Alloy Information provided by MRC Polymers Inc. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
Glastic Laminates/Shapes SG-200 High Strength/High Temperature Polyester Laminate Data provided by Glastic Corporation.NEMA GPO-1. A superior replacement for epoxy-bonded mica in layer insulation applications. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D256 |
Multibase Multi-Flamâ„¢ 2602 PP Polypropylene Features:Flame RetardantHalogenatedBlooming, None Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | 73°F; ASTM D256 |
Spartech Royalite R52 PVC/Acrylic Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
Star Plastics PC1212FRR Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
unfilled; ASTM D256 |
Shuman 910-05V0 Utility Black Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 7001 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® PPC300NB-10M Utility Polypropylene Copolymer Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D256 |
Lubrizol ESTALOC® 59010 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas and AsiaInformation provided by Lubrizol |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers DIAMALOY 527 PC/PBT Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr.. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® PPC100-20M Polypropylene Copolymer Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics PC2200 PC PC2200 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |