| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 81 | 81 | ASTM D2240 |
| Tensile Strength, Yield | 47.6 MPa | 6900 psi | Type I, 51 mm/min; ASTM D638 |
| Elongation at Break | 13 % | 13 % | Type I, 51 mm/min; ASTM D638 |
| Tensile Modulus | 2.53 GPa | 367 ksi | Type I, 51 mm/min; ASTM D638 |
| Flexural Strength | 80.7 MPa | 11700 psi | ASTM D790 |
| Flexural Modulus | 2.92 GPa | 424 ksi | ASTM D790 |
| Izod Impact, Notched | 6.40 J/cm <br>@Thickness 3.18 mm,<br> Temperature 23.0 °C |
12.0 ft-lb/in <br>@Thickness 0.125 in,<br> Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 61.1 °C <br>@Thickness 3.18 mm |
142 °F <br>@Thickness 0.125 in |
Unannealed; ASTM D648 |
| 67.8 °C <br>@Thickness 3.18 mm |
154 °F <br>@Thickness 0.125 in |
Annealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 55.6 °C <br>@Thickness 3.18 mm |
132 °F <br>@Thickness 0.125 in |
Unannealed; ASTM D648 |
| 63.3 °C <br>@Thickness 3.18 mm |
146 °F <br>@Thickness 0.125 in |
Annealed; ASTM D648 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | High Flow | |
| High Impact Resistance | ||
| Forms | Pellets | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Processing Method | Injection Molding | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Decorative Parts | |
| General Purpose | ||
| Outdoor Applications |