Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.540 - 1.90 J/cm @Temperature -40.0 - -20.0 °C |
1.01 - 3.56 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 1.21 J/cm Grade Count:12 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Notched | 0.540 J/cm @Temperature -30.0 °C |
1.01 ft-lb/in @Temperature -22.0 °F |
|
Asahi Kasei Tenac®-C 4510 Acetal Copolymer, General Purpose
(discontinued **) General-purpose grade, characterized by balanced flowability and mechanical properties.Applications: Gears, cams, hose joints, clips, switches, mechanical parts of audio and video equipment.This pro.. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
Firestone C200-001 Nylon 6 Natural color. Not heat stabilized, modified, or lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
Firestone CL200-001 Nylon 6 Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
LG Chemical HI855HS PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |
|||
Izod Impact, Notched | 0.539 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.01 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUCEL N145LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
Kolon KOCETAL® LW301 Wear Modified Acetal Resin Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
Kolon KOPA® KN333HB40HFBL Hybrid Nylon 66 High flow, dimensionally stableApplications Fans & ShroudsInformation provided by API-Kolon. |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | Low Temp |
Kolon KOPEL® KP3372 General Purpose TPE Resin KOPEL® is a thermoplastic polyester elastomer which is a new engineering rubber having combined properties of conventional rubber and thermoplastic. Its flexibility and elastic recovery are very.. |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | DIN 53453; ASTM D256 |
Kolon NOPLA® KE831 PEN-PET Copolyester NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac.. |
|||
Izod Impact, Notched | 0.539 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.01 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP1000H PBT Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.539 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.01 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® SG5200 PBT+PET+GF20% Description: Injection Molding, PBT+PET+GF20%, Good Surface Application: E&E (Microwave Oven Door Gasket)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.539 J/cm @Temperature 23.0 °C |
1.01 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC R1610 Polypropylene Random Copolymer Features: SEETEC R1610 is a highly transparent ethylene-propylene random copolymer for injection molding applications. SEETEC R1610 exhibits an excellent transparency and a good impact strength. SEE.. |
|||
Izod Impact, Notched | >= 0.539 J/cm @Thickness 6.35 mm |
>= 1.01 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 1100-211H Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Izod Impact, Notched | >= 0.540 J/cm | >= 1.01 ft-lb/in | Reversed Notch (Method E); ASTM D 256 |
Karina E 854-35/1-Y-ERYB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | >= 0.539 J/cm @Thickness 6.35 mm |
>= 1.01 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 2100-104B Product Description: PBT unreinforced flame-retarded injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellen.. |
|||
Izod Impact, Notched | >= 0.539 J/cm @Thickness 6.35 mm |
>= 1.01 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 3020-104 15% Glass Fiber Filled Product Description: A glass fiber 20% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC (Asia Pacific) Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys.. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KFI12 Acetal Copolymer LNP LUBRICOMP* KFI12 is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
UBE UBESTA® 3020X8 Nylon 12 Thermister Description: UBESTA Nylon 12 ThermisterInformation provided by UBE. |
|||
Izod Impact, Notched | 0.540 J/cm @Thickness 3.17 mm |
1.01 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Unitika AXF-1500-05 Dry Characteristics: Lubricant grade of AX1500, excellent in heat and chemical resistancesInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | ASTM D256 |
Cheng Yu Plastic N6C2 Nylon 6, 20% Mineral Reinforced |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | ASTM D256 |
Cheng Yu Plastic NGCV2 Flame Retardant Nylon 6, 20% Mineral Reinforced |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® TA210MS MoS2 Filled PA66 Resin Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.T-series: Impact modified,.. |
|||
Izod Impact, Notched | 0.540 J/cm @Thickness 3.17 mm |
1.01 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Entec Hypro™ PPC-T40 Copolymer Polypropylene, 40% Talc Reinforced Information provided by Entec |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | Dry; ASTM D256 |
Asahi Kasei Leona® 9400S Nylon 66 Excellent impact resistance. Suitable for thick-wall parts.Applications:Railroad tie insulatorsInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 195-N2 Acetal A general purpose, medium viscosity natural.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.540 J/cm @Temperature -40.0 °C |
1.01 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Ashley Polymers Ashlene® 279 PPO Alloy A general purpose, paintable injection molding grade with high chemical resistance and mechanical performance. Good heat resistance with dimensional stability in dark gray or black only.Data provid.. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® R195B Acetal A general purpose, low viscosity with excellent toughness, strength, stiffness, lubricity in black. Available in UV stabilized grades: R195-B2 (good weatherability); R195-HB2 (maximum weatherabili.. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
Plenco 50335 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.Inform.. |