Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Mineral Filled
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic N6C2 Nylon 6, 20% Mineral Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Water Absorption 0.20 %
0.20 %
ASTM D570
Linear Mold Shrinkage 0.0080 - 0.015 cm/cm
0.0080 - 0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 90
90
ASTM D785
Tensile Strength, Yield 73.5 MPa
10700 psi
ASTM D638
Flexural Yield Strength 127 MPa
18500 psi
ASTM D790
Izod Impact, Notched 0.539 J/cm
1.01 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 226 °C
439 °F
ASTM D648
Flammability, UL94 HB
HB