Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.420 - 0.480 J/cm | 0.787 - 0.899 ft-lb/in | ASTM D256 |
Huntsman RenShape® SL 7820 Stereolithography Plastic RenShape® SL 7820 stereolithography material is a white, low viscosity and stable liquid that produces strong black models and prototypes with good surface fi nish and detail, and ABS-like appear.. |
|||
Izod Impact, Notched | >= 0.420 J/cm | >= 0.787 ft-lb/in | Method A; ASTM D 256 |
Karina E 835-10/155-C-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | >= 0.420 J/cm | >= 0.787 ft-lb/in | Method A; ASTM D 256 |
Karina E 835-18/115-C-ERYB Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP IAL12 PA 6/12 (Asia Pacific) LNP* Lubricomp* IAL12 is a compound based on Nylon 6/12 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KFL32R Acetal Copolymer LNP LUBRICOMP* KFL32R is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 15% PTFE. Added feature of this material is: Easy Release, Wear Resistant. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copoly (Asia Pacific) LNP* Lubricomp* KL004L is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer (Asia Pacific) LNP Lubricomp* KL004U is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. This grade was previously found under the LNP* F.. |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature 23.0 °C |
0.787 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Am.. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 771 PBT 35% mineral/glass reinforced flame retardant grade with a CTI performance level class of 0 rating. Applications which may see electrical arcing. |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature 23.0 °C |
0.787 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon EE006EM PEI (Asia Pacific) LNP* Stat-kon* EE006EM is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by .. |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature 23.0 °C |
0.787 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon KS302 Acetal Copoly LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC3508 PPE+HIPS (Europe-Africa-Middle East) PRELIMINARY DATA. LNP* Stat-kon* Noryl_NC3508 compound is a 33% glass/mineral/carbon filled PPE+PS. ESD, high heat, tight tolerance: electronic packaging/chip trays. |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature 23.0 °C |
0.787 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon RX89129 PA 66 LNP* Stat-Kon RX89129 is a compound based on Nylon 6,6. Fillers are proprietary.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP PF003 PA 6 LNP THERMOCOMP* PF003 is a compound based on Nylon 6 resin containing 15% Glass Fiber. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66 (Asia Pacific) LNP* Thermocomp* RF0029S is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature 23.0 °C |
0.787 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp RFZ71S PA 66 (Asia Pacific) LNP* Thermocomp* RFZ71S is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for t.. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP WF006U PBT (Asia Pacific) LNP* THERMOCOMP* WF006U is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: UV Stabilized. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX RNX130 PPE+PS+PA 30% glass reinforced PPE+PS+PA alloy for automotive and nonautomotive applications. Recycle grade in black/gray only. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP JX91198 PES LNP LUBRICOMP* JX91198 is a compound based on Polyethersulfone resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON KE002 ACETAL LNP* STAT-KON* KE002 is a compound based on Acetal resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® FXV310SK PBT VALOX FXV310SK is an unreinforced PBT injection moulding Visualfx* resin with high flow characteristics and containing a metal sparkle. Applications: automotive bezels and appliances. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East) 6.5% glass reinforced, Super High Flow, flame retardant PBT. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DB008ERP PC LNP* THERMOCOMP* DB008ERP is a compound based on Polycarbonate resin containing 40% Glass Bead. Added features of this material include: Easy Molding, Mold Release. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DB008ERP PC (Asia Pacific) LNP* Thermocomp* DB008ERP is a compound based on Polycarbonate resin containing Glass Bead. Added features of this material include: Easy Molding, Mold Release. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF002 PA 66 LNP THERMOCOMP* RF002 is a compound based on Nylon 66 resin containing 10% Glass Fiber. |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature 23.0 °C |
0.787 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermotuf VFM53 PA 66 LNP THERMOTUF* VFM53 is a compound based on Nylon resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas.. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3715 Glass Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 3715 is a 15% glass filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256A |
Total PPH 3281 Polypropylene, Extrusion Grade Low melt flow homopolymer for sheet extrusion, strapping, and in-line thermoforming applicationsMelt Strength – The high melt strength of FINA 3281 allows uniform drawdown during processing, result.. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3715 Glass Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 3715 is a 15% glass filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP PH0460A PA 6 (Asia Pacific) LNP* Thermocomp* PH0460A is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |