Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.650 - 0.800 J/cm | 1.22 - 1.50 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ RGD5160-DM ABS-like Prototyping Polymer Objet ABS-like Digital Material made of Object RGD515 & Objet RGD535Digital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to.. |
|||
Izod Impact, Notched | 0.481 - 0.800 J/cm | 0.900 - 1.50 ft-lb/in | Average value: 0.540 J/cm Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an.. |
|||
Izod Impact, Notched | 0.350 - 0.800 J/cm | 0.656 - 1.50 ft-lb/in | Average value: 0.575 J/cm Grade Count:15 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched | 0.350 - 0.800 J/cm @Temperature -40.0 - 0.000 °C |
0.656 - 1.50 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 0.531 J/cm Grade Count:6 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Izod Impact, Notched | 0.480 - 0.800 J/cm @Thickness 6.35 mm |
0.899 - 1.50 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ ATH-000/02T Homopolymer - 2% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.530 - 0.800 J/cm @Thickness 6.35 mm |
0.993 - 1.50 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ ATH-000/05M Acetal Homopolymer - 5% MoS2
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.600 - 0.800 J/cm @Temperature -40.0 - 0.000 °C |
1.12 - 1.50 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 0.642 J/cm Grade Count:1 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Izod Impact, Notched | 0.600 - 0.800 J/cm @Thickness 3.20 - 3.20 mm |
1.12 - 1.50 ft-lb/in @Thickness 0.126 - 0.126 in |
Average value: 0.642 J/cm Grade Count:1 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Izod Impact, Notched | 0.374 - 0.800 J/cm | 0.700 - 1.50 ft-lb/in | Average value: 0.527 J/cm Grade Count:4 |
Overview of materials for Polyamide-Imide, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Notched | 0.530 - 0.800 J/cm @Thickness 6.35 mm |
0.993 - 1.50 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Edgetek® LCP-30CF/000 Liquid Crystal Polymer - 30% Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.108 - 0.800 J/cm | 0.202 - 1.50 ft-lb/in | Average value: 0.345 J/cm Grade Count:18 |
Overview of materials for Cyclo Olefin Polymer This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Izod Impact, Notched | 0.758 - 0.800 J/cm | 1.42 - 1.50 ft-lb/in | Average value: 0.786 J/cm Grade Count:3 |
Overview of materials for Polychlorotrifluoroethylene; Molded This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Notched | 0.720 - 0.800 J/cm @Temperature -40.0 - -40.0 °C |
1.35 - 1.50 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.760 J/cm Grade Count:1 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Izod Impact, Notched | 0.600 - 0.800 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.12 - 1.50 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM PA 66 GF 30 Polyamide 66, 30% Glass Characteristics: 30% glass fibre filled |
|||
Izod Impact, Notched | 0.42712 - 0.800 J/cm @Temperature -17.8 - 0.000 °C |
0.80017 - 1.50 ft-lb/in @Temperature 0.000 - 32.0 °F |
Average value: 0.614 J/cm Grade Count:2 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 0.270 - 0.800 J/cm @Temperature -40.0 - -40.0 °C |
0.506 - 1.50 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.447 J/cm Grade Count:11 |
Overview of materials for Ethyl Cellulose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ethyl Cellulose, Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Izod Impact, Notched | 0.374 - 0.800 J/cm | 0.700 - 1.50 ft-lb/in | Average value: 0.544 J/cm Grade Count:7 |
Overview of materials for Polypropylene with Glass Fiber + Bead Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Notched | 0.800 - 0.800 J/cm @Temperature -40.0 - -40.0 °C |
1.50 - 1.50 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.800 J/cm Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Izod Impact, Notched | 0.600 - 0.800 J/cm @Temperature 0.000 - 0.000 °C |
1.12 - 1.50 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 0.468 J/cm Grade Count:4 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 0.26695 - 0.800 J/cm @Temperature 0.000 - 0.000 °C |
0.50011 - 1.50 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 0.516 J/cm Grade Count:3 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.26695 - 0.800 J/cm @Diameter 6.35 - 6.35 mm |
0.50011 - 1.50 ft-lb/in @Diameter 0.250 - 0.250 in |
Average value: 0.516 J/cm Grade Count:3 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.350 - 0.800 J/cm @Temperature -40.0 - 0.000 °C |
0.656 - 1.50 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 0.533 J/cm Grade Count:4 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |