Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.71 J/cm @Temperature 23.0 °C |
3.20 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products GC10P200-00 10% Glass Fiber Reinforced Polypropylene Copolymer, Non-UV Stabilized, Chemically Coupled, Natural Applications: Component housingsStorage binsRecreational vehicle trim and bumpersInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | 73°F; ASTM D256 |
Ravago Manufacturing Americas Hylon® N1043HL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Izod Impact, Notched | 1.71 J/cm @Thickness 3.18 mm |
3.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® UF-1009 HS Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | Injection Molding; ASTM D256 |
Network Polymers 707 Polystyrene Description: Ignition RetardantInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM Data |
Americas Styrenics Styron® XL-8028 High Impact Polystyrene
(discontinued **) STYRON® XL-8028 high impact polystyrene is designed for VCR cassettes, toys, small appliances, telephones, housewares, tool items, computer consoles and bodies for computer cartridges. It offers hi.. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFI14 PC LNP* Lubricomp* DFI14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 2% Silicone. Added features include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.71 - 3.74 J/cm | 3.20 - 7.01 ft-lb/in | Average value: 2.30 J/cm Grade Count:5 |
Overview of materials for Nylon 12, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Izod Impact, Notched | 1.71 J/cm @Thickness 3.20 mm |
3.20 ft-lb/in @Thickness 0.126 in |
ASTM-D256 |
Ineos ABS Lustran® 308 ABS, Medical Grade Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resi.. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256A |
Ineos Styrenics Avantra® 597N Polystyrene (NAFTA) High-impact grade of polystyrene with improved impact strength and heat resistance, developed for injection molding and extrusion/thermoforming applications.Information provided by BASF.Ineos Styren.. |
|||
Izod Impact, Notched | 1.71 J/cm @Thickness 3.17 mm |
3.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Lucent Polymers GPP-330 Polypropylene, 30% Glass Fiber Reinforced, Chemically Coupled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | 0.125 in; ASTM D256 |
Chase Plastics CP Pryme® A100HF ABS Features: High FlowGeneral PurposeGood toughnessForm: PelletsInformation provided by Chase Plastics. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® A100HF ABS Molding Resin, High Flow Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 6 GF15H 15% Glass Fiber Reinforced, Heat Impact Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.71 - 2.40 J/cm | 3.20 - 4.50 ft-lb/in | ASTM D256 |
Westlake Plastics Ultra Ethylux® HDPE Ultra Ethylux is made from high density polyethylene resin. This material is a cost effective alternative for a variety of end uses including mild chemical and wear applications. Information provid.. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 6 GF15H 15% Glass Fiber Reinforced, Heat Impact Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® GFRMPPCC-10 10% Glass Reinforced Polypropylene, High Impact Polifil® GFRMPPCC series compounds are high impact polypropylenes reinforced with chemically coupled glass fibers. This combination provides higher impact strength while retaining high stiffness.Ap.. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256A |
ExxonMobil PP7855E1 Polypropylene Homopolymer Product Description: A high crystallinity, medium impact strength copolymer resin with high melt flow rate and good processing attributes. It is designed for injection-molded automotive interior ap.. |
|||
Izod Impact, Notched | 1.71 J/cm @Temperature 22.8 °C |
3.20 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol PA233G13 Nylon 6, 13% Glass Fiber, Improved Processability, Easily Colorable, Toughened Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 1.71 J/cm @Temperature 22.8 °C |
3.20 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol PA233G13HT Nylon 6, 13% Glass Fiber, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0437W20L Wollastonite Reinforced |
|||
Izod Impact, Notched | 1.71 J/cm @Thickness 3.17 mm |
3.20 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® 7523-2AM BK ND3007 33% Glass Filled PA66 (Dry) Ultramid 7523-2AM BK ND3007 is an impact modified, 33% glass reinforced, heat stabilized injection molding PA6/6. |
|||
Izod Impact, Notched | 1.71 J/cm @Thickness 3.17 mm |
3.20 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® 8202C PA6 (Conditioned) Ultramid 8202C is a modified crystalline and low viscosity, nylon 6 injection molding homopolymer. It is also available in heat stabilized (Ultamid 8202C HS) and/or pigmented versions. Its unique .. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 514 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 279 PPO Alloy A general purpose, paintable injection molding grade with high chemical resistance and mechanical performance. Good heat resistance with dimensional stability in dark gray or black only.Data provid.. |
|||
Izod Impact, Notched | 1.71 J/cm @Temperature 22.8 °C |
3.20 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Teknor Apex Sinelec CCB6814 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Electrically Conductive Uses: Corrugated Sheet Forms: Pellets Processing Method: Injection Method; Sheet Extr.. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256 Type A |
Quadrant EPP Quadrant CPVC - ASTM D1748, Cell Classification (ASTM Product Data Sheet) |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256 |
Ineos Nova Zyntar® 707 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |