Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® A100HF ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Chase Plastics CP Pryme® A100HF ABS.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: High FlowGeneral PurposeGood toughnessForm: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Melt Flow 7.95 g/10 min
7.95 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Elongation at Break 7.0 %
7.0 %
ASTM D638
Flexural Yield Strength 80.0 MPa
11600 psi
ASTM D790
Flexural Modulus 2.85 GPa
413 ksi
ASTM D790
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
0.125 in; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.9 °C
192 °F
Unannealed, 0.125 in; ASTM D648
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: