Category | Polymer , Thermoplastic , Vinyl (PVC) , Chlorinated PVC (CPVC) |
Manufacturer | Quadrant Engineering Plastics Products |
Trade Name | Quadrant |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Quadrant EPP Quadrant CPVC - ASTM D1748, Cell Classification (ASTM Product Data Sheet).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.56 g/cc | 1.56 g/cc | ASTM D792 |
Water Absorption | <= 0.040 % | <= 0.040 % | Immersion, 24hr; ASTM D570(2) |
Water Absorption at Saturation | <= 0.040 % | <= 0.040 % | Immersion; ASTM D570(2) |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore D | 84 | 84 | ASTM D2240 |
Tensile Strength | 42.4 MPa | 6150 psi | ASTM D638 |
Elongation at Break | 12 % | 12 % | ASTM D638 |
Tensile Modulus | 1.79 GPa | 260 ksi | ASTM D638 |
Flexural Strength | 46.2 MPa | 6700 psi | ASTM D790 |
Flexural Modulus | 2.68 GPa | 388 ksi | ASTM D790 |
Compressive Strength | 96.5 MPa | 14000 psi | 10% Def.; ASTM D695 |
Compressive Modulus | 2.41 GPa | 350 ksi | ASTM D695 |
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256 Type A |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 93.3 °C | 200 °F | Long Term |
Deflection Temperature at 1.8 MPa (264 psi) | 46.7 °C | 116 °F | ASTM D648 |
Flammability, UL94 | V-0 | V-0 | 1/8 inch (Estimated Rating) |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.00e+12 ohm | >= 1.00e+12 ohm | ASTM D257 |
Compliance Properties | Metric | English | Comments |
---|---|---|---|
3A-Dairy | No | No | |
Canada AG | No | No | |
FDA | No | No | |
NSF | Yes | Yes | STD 14 & 61 |
USDA | No | No | |
USP Class VI | No | No |
Chemical Resistance Properties | Metric | English | Comments |
---|---|---|---|
Acids, Strong (pH 1-3) | Limited | Limited | |
Acids, Weak | Acceptable | Acceptable | |
Alcohols | Acceptable | Acceptable | |
Alkalies, Strong (pH 11-14) | Acceptable | Acceptable | |
Alkalies, Weak | Acceptable | Acceptable | |
Chlorinated Solvents | Limited | Limited | |
Conductive / Static Dissipative | Yes | Yes | |
Continuous Sunlight | Limited | Limited | |
Hot Water / Steam | Limited | Limited | |
Hydrocarbons - Aliphatic | Limited | Limited | |
Hydrocarbons - Aromatic | Limited | Limited | |
Inorganic Salt Solutions | Acceptable | Acceptable | |
Ketones, Esters | Unacceptable | Unacceptable |
Descriptive Properties | Value | Comments |
---|---|---|
Color | Grey | |
Machinability | 6 | 1-10, 1=Easier to Machine |