Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CY6009 PC+ABS (Asia Pacific) CY6009 is a flame retardant (FR) PC+ABS blend with non-brominated and non-chlorinated FR systems. Its excellent flow together with balanced properties and thin wall 5VB capability at less than 2 mm.. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HP1HF PC Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Europe-Africa-Middle East) XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | ASTM D256 type "A" |
Technetics Group Amicon™ PEEK 30% Carbon
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | ASTM D256 |
SABIC PP 623B Polypropylene Random Co-polymer for Cast Film Product Description: PP 623B is a PP Random Copolymer grade specially designed for Cast PP (CPP) film extrusion. It contains slip agent and anti-block additives. PP 623B offers good heat weldabil.. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HP1HF PC (Asia Pacific) Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Izod Impact, Notched | 0.550 - 0.834 J/cm | 1.03 - 1.56 ft-lb/in | Average value: 0.714 J/cm Grade Count:3 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Izod Impact, Notched | 0.550 - 1.50 J/cm | 1.03 - 2.81 ft-lb/in | Average value: 1.04 J/cm Grade Count:4 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Izod Impact, Notched | 0.550 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.03 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PBT-T15 15% Mineral Filled PBT Features:Excellent size stabilityLow tendency to wrapLow abrasionGood surfaceApplications:Injection moldingApplication partsE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Izod Impact, Notched | 0.550 - 0.600 J/cm | 1.03 - 1.12 ft-lb/in | ASTM D256 |
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:.. |
|||
Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem PCC 4414 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36F PPS - Linear LNP LUBRICOMP* OCP36F is a compound based on PPS - Linear resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Bearing Grade, Electrically Conductive, Wear R.. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM ATX200R PEI Blend (Europe-Africa-Middle East) High flow Polyetherimide blend with internal mold release. RoHS compliant. UL94 V0 Listing. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL N300X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL N300X PPE+PS (Asia Pacific) PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
A. Schulman POLYTROPE™ TPP 1024E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1024E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |
|||
Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1434 Couple Mica In Copolymer Polypropylene (25% Mineral Filled) DescriptionPolyfort® FPP 1434 is a 25% coupled mica copolymer polypropyleneInformation provided by A. Schulman. |
|||
Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1434 Couple Mica In Copolymer Polypropylene (25% Mineral Filled) DescriptionPolyfort® FPP 1434 is a 25% coupled mica copolymer polypropyleneInformation provided by A. Schulman. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature 23.0 °C |
1.03 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTough PZ301R8 Polycarbonate, 40% Carbon Fiber 40% Carbon fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1434 Couple Mica In Copolymer Polypropylene (25% Mineral Filled) DescriptionPolyfort® FPP 1434 is a 25% coupled mica copolymer polypropyleneInformation provided by A. Schulman. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature 23.0 °C |
1.03 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PA100 Nylon 6.6, General Purpose General purpose polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | >= 0.550 J/cm @Temperature 23.0 °C |
>= 1.03 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek RA102 Nylon 6.6, General Purpose General purpose polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature 23.0 °C |
1.03 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTal PM1409 Acetal, PTFE Filled Polyacetal filled with PTFE for sliding parts, low friction and improved wear resistance in molded parts.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | ASTM D256A |
DSM Somos® 9110 Epoxy Photopolymer DescriptionDSM Somos® 9110 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance, a wide p.. |
|||
Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | ASTM D256 |
Ensinger Tecapeek® XP-98 Compression Molded PEEK Compound, 30% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Izod Impact, Notched | 0.550 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.03 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM PA 6/66 GF 30 Polyamide 6/66, 30% Glass Characteristics: 30% glass fibre filled |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ISO 180/A |
BASF Ultraform N 2310P Q600 POM Ultraform N2310P Q600 is a general-purpose injection molding POM grade containing special lubricant. Low frictional coefficient giving extremely low wear with otherwise unaltered mechanical propert.. |
|||
Izod Impact, Notched | 0.550 J/cm @Thickness 3.17 mm |
1.03 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® 8267G HS BK-106A 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-106A is a heat stabilized, weather resistant, 40% mineral and glass fiber reinforced PA6 injection molding compound with improved UV resistance and sink mark resistance. The co.. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
A. Schulman POLYTROPE™ TPP 1024E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1024E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |
|||
Izod Impact, Notched | 0.550 - 0.650 J/cm | 1.03 - 1.22 ft-lb/in | ASTM D256 |
Loxim 830 01 HB Polypropylene Compound, Flame Retardant Information provided by Loxim Industries |