Material Notes:
DescriptionDSM Somos® 9110 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance, a wide processing latitude and excellent tolerance to a broad temperature and humidity range during and after build. Parts created from Somos® 9110 exhibit superior fatigue properties, strong memory retention and high quality up-facing and down-facing surfaces. Somos® 9110 also offers a good balance of properties between rigidity and functionality. The resulting part properties are ideal for master patterns in rubber molding applications. This material is also useful in creating parts for applications where durability and robustness are critical requirements (e.g. automobile components, electronic housings, medical products, large panels and snap-fit parts).ApplicationSomos® 9110 Photopolymer is used in the solid imaging process to build three-dimensional parts.Information Provided by DSM Desotech Inc.
Physical Properties Metric English Comments
Density 1.13 g/cc

@Temperature 25.0 °C
0.0408 lb/in³

@Temperature 77.0 °F
Viscosity 230 cP

@Temperature 30.0 °C
230 cP

@Temperature 86.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 83
83
ASTM D2240
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638M
Elongation at Yield 15 - 21 %
15 - 21 %
ASTM D638M
Modulus of Elasticity 1.59 GPa
231 ksi
ASTM D638M
Flexural Strength 44.0 MPa
6380 psi
ASTM D790M
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790M
Izod Impact, Notched 0.550 J/cm
1.03 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °C
122 °F
ASTM D648
Descriptive Properties Value Comments
Appearance Transparent Amber
Dp (mm) 0.132
Slope of cure-depth vs. ln(E) curve
E10 (mJ/cm2) 55
Exposure that gives 0.254mm thickness
Ec (mJ/cm2) 8
Critical exposure