Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.390 J/cm | 0.731 ft-lb/in | ASTM D256A |
LyondellBasell Pro-fax 6523 Polypropylene Homopolymer, General Purpose Key Features: general purpose polypropylene homopolymer resin, stiff, high resistance to solvents, FDA acceptableApplications: automotive, hospital and institutional ware, housewares, general moldin.. |
|||
Izod Impact, Notched | 0.390 J/cm | 0.731 ft-lb/in | ASTM D256 |
LG Chemical LUCON PO-3000 Electrically Conductive Thermoplastic LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Izod Impact, Notched | 0.390 J/cm | 0.731 ft-lb/in | ASTM D256 |
LG Chemical LUCON SE-4200H Electrically Conductive Thermoplastic LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Izod Impact, Notched | 0.390 J/cm @Temperature 23.0 °C |
0.731 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOS HR-2307 Heat Resistant SAN, 30% Glass Fiber Reinforced LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Izod Impact, Notched | 0.390 J/cm | 0.731 ft-lb/in | ASTM D256 |
Kaneka PHBH Semi-Rigid Bio-based Polymer A copolymer produced of 3-hydroxybutyrate and 3-hydroxyhexanoate produced by fermentation of plant oils. It has excellent biodegradability (under anaerobic, aerobic, aquatic, and compost conditions.. |
|||
Izod Impact, Notched | >= 0.390 J/cm | >= 0.731 ft-lb/in | Method A; ASTM D 256 |
Karina E 830-10/150-Y-ERYB-LMP White PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | >= 0.390 J/cm | >= 0.731 ft-lb/in | Method A; ASTM D 256 |
Karina E 830-35/1-Y-ERYB-LMP Ivory PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles/.p>Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | >= 0.390 J/cm | >= 0.731 ft-lb/in | Method A; ASTM D 256 |
Karina E 832-35/1-Y-ERA-LMP Ivory PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | >= 0.390 J/cm | >= 0.731 ft-lb/in | Method A; ASTM D 256 |
Karina E 834-35/1-Y-ERA-LMP Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | 0.390 J/cm | 0.731 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP FL003 PE LNP* LUBRICOMP* FL003 is a compound based on Polyethylene resin containing 15% PTFE. Added features include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.390 J/cm | 0.731 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KFP032 Acetal Copolymer LNP LUBRICOMP* KFP032 is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 0.390 J/cm | 0.731 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP QL002 PA 6/10 LNP* LUBRICOMP* QL002 is a compound based on Nylon 6/10 containing 10% PTFE. Added features of this grade are: Wear Resistant. |
|||
Izod Impact, Notched | 0.390 J/cm | 0.731 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP QL004 PA6.10 LNP* LUBRICOMP* QL004 is a compound based on Nylon 6/10 containing 20% PTFE. Added features of this grade include: Wear Resistant. |
|||
Izod Impact, Notched | 0.390 J/cm | 0.731 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 2312EPR PEI 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Izod Impact, Notched | 0.390 J/cm | 0.731 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 2312EPR PEI (Asia Pacific) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Izod Impact, Notched | 0.390 J/cm @Temperature 23.0 °C |
0.731 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 2312EPR PEI (Europe-Africa-Middle East) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Izod Impact, Notched | 0.390 J/cm @Temperature 23.0 °C |
0.731 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® TS4016 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.390 J/cm | 0.731 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF003AXH PA 66 LNP* THERMOCOMP* RF003AXH is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this material includes: Healthcare. |
|||
Izod Impact, Notched | 0.390 J/cm | 0.731 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Asia Pacific) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Izod Impact, Notched | 0.390 J/cm | 0.731 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX675 PPE+PA6 Noryl GTX* GTX675 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to a.. |
|||
Izod Impact, Notched | 0.390 J/cm | 0.731 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Izod Impact, Notched | 0.390 J/cm | 0.731 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Europe-Africa-Middle East) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Izod Impact, Notched | 0.390 J/cm | 0.730 ft-lb/in | ASTM D256 |
Teknor Apex Sinvicomp SRF 9702/C Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Medium Impact Resistance Uses: Electrical/Electronic Applications Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Izod Impact, Notched | 0.390 J/cm | 0.730 ft-lb/in | ASTM D256 |
Teknor Apex Sinvicomp SRP 9613 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good Impact Resistance Uses: Profiles Forms: Granules Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Izod Impact, Notched | 0.390 J/cm @Temperature 23.0 °C |
0.731 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem H 605 Thermoforming Polypropylene Applications: Flat and corrugated sheets with high transparency; thermoformed packing with high transparency. Information provided by Braskem |
|||
Izod Impact, Notched | 0.390 J/cm | 0.731 ft-lb/in | Dry; ASTM D256 |
Asahi Kasei Leona® 1300S Nylon 66 General purpose grade. Good balance of flowability and mechanical properties.Applications:Connectors, washers, cable ties. Information provided by Asahi Kasei |
|||
Izod Impact, Notched | 0.390 J/cm | 0.731 ft-lb/in | Wet; ASTM D256 |
Asahi Kasei Leona® CR301 Nylon 66 Suitable for a switch insulator. Low abrasion and superior electrical properties.Applications:Sliding switch insulators Information provided by Asahi Kasei |
|||
Izod Impact, Notched | 0.390 J/cm | 0.730 ft-lb/in | ASTM D256 |
Teknor Apex Sinvicomp DBS 8615 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good Impact Resistance Uses: Piping Forms: Powder Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Izod Impact, Notched | 0.390 J/cm | 0.731 ft-lb/in | ASTM D256 |
Plenco 51015 PET, Pellet, Injection Molded, Black