Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.500 - 0.500 J/cm² @Temperature -30.0 - -30.0 °C |
2.38 - 2.38 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.500 J/cm² Grade Count:1 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact, Notched | 0.300 - 0.500 J/cm² | 1.43 - 2.38 ft-lb/in² | Average value: 0.435 J/cm² Grade Count:10 |
Overview of materials for Acetal Copolymer, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Charpy Impact, Notched | 0.250 - 0.500 J/cm² | 1.19 - 2.38 ft-lb/in² | Average value: 0.360 J/cm² Grade Count:6 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Charpy Impact, Notched | 0.340 - 0.500 J/cm² | 1.62 - 2.38 ft-lb/in² | Average value: 0.413 J/cm² Grade Count:3 |
Overview of materials for Phenolic, Resole, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Charpy Impact, Notched | 0.390 - 0.500 J/cm² @Temperature -30.0 - -20.0 °C |
1.86 - 2.38 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.430 J/cm² Grade Count:3 |
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu.. |
|||
Charpy Impact, Notched | 0.500 - 0.500 J/cm² @Temperature -30.0 - -30.0 °C |
2.38 - 2.38 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.500 J/cm² Grade Count:1 |
Overview of materials for Nylon 66, Film This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Film". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Charpy Impact, Notched | 0.400 - 0.500 J/cm² @Temperature -40.0 - -20.0 °C |
1.90 - 2.38 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 0.450 J/cm² Grade Count:2 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |
|||
Charpy Impact, Notched | 0.500 - 0.500 J/cm² @Temperature -30.0 - -30.0 °C |
2.38 - 2.38 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.500 J/cm² Grade Count:8 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Charpy Impact, Notched | 0.200 - 0.500 J/cm² @Temperature -20.0 - 30.0 °C |
0.952 - 2.38 ft-lb/in² @Temperature -4.00 - 86.0 °F |
Average value: 0.350 J/cm² Grade Count:5 |
Overview of materials for Nylon 66/6, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact, Notched | 0.300 - 0.500 J/cm² @Temperature -30.0 - -30.0 °C |
1.43 - 2.38 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.447 J/cm² Grade Count:6 |
Overview of materials for Nylon 66, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Charpy Impact, Notched | 0.150 - 0.500 J/cm² | 0.714 - 2.38 ft-lb/in² | Average value: 0.278 J/cm² Grade Count:9 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact, Notched | 0.300 - 0.500 J/cm² | 1.43 - 2.38 ft-lb/in² | Average value: 0.433 J/cm² Grade Count:3 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Charpy Impact, Notched | 0.500 - 0.500 J/cm² @Temperature -30.0 - -30.0 °C |
2.38 - 2.38 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.500 J/cm² Grade Count:1 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Charpy Impact, Notched | 0.350 - 0.500 J/cm² | 1.67 - 2.38 ft-lb/in² | Injection; ISO 179/1eA |
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc.. |
|||
Charpy Impact, Notched | 0.300 - 0.500 J/cm² | 1.43 - 2.38 ft-lb/in² | Injection; ISO 179/1eA |
Raschig Group DECAL® 152CL Phenolic Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet.. |
|||
Charpy Impact, Notched | 0.350 - 0.500 J/cm² | 1.67 - 2.38 ft-lb/in² | Compression; ISO 179/1eA |
Raschig Group RALUPOL® 8605 UP Polyester Glass fiber reinforced polyester molding compound. Resistant to hydrolysis. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU dire.. |
|||
Charpy Impact, Notched | 0.300 - 0.500 J/cm² | 1.43 - 2.38 ft-lb/in² | Injection; ISO 179/1eA |
Raschig Group RESINOL® 400 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Charpy Impact, Notched | 0.200 - 0.500 J/cm² @Temperature -20.0 - -20.0 °C |
0.952 - 2.38 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 0.340 J/cm² Grade Count:5 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Charpy Impact, Notched | 0.150 - 0.500 J/cm² | 0.714 - 2.38 ft-lb/in² | Average value: 0.317 J/cm² Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |
|||
Charpy Impact, Notched | 0.270 - 0.500 J/cm² @Temperature -30.0 - -30.0 °C |
1.28 - 2.38 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.345 J/cm² Grade Count:4 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |