Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Geloy XTWM200 ASA ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Geloy XTWM200 ASA (Asia Pacific) ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Asia Pacific) Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
PolyOne Bergamid™ A70 G50 HW SO Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® LUX9136C PC COPOLYMER (Asia Pacific) Lexan* LUX9136C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | Matt/Matt, Matt side impacted; ISO 179-1/fa |
Polycasa HIPS QUINN HIPS is a rubber modified polystyrene sheet that has improved impact strength and is easy to mould and cut to size. The product is available with either a matt finish on both sides or a matt f.. |
|||
Charpy Impact, Notched | 1.00 - 1.50 J/cm² @Temperature -30.0 - -30.0 °C |
4.76 - 7.14 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.33 J/cm² Grade Count:2 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
Charpy Impact, Notched | 1.00 - 5.40 J/cm² | 4.76 - 25.7 ft-lb/in² | Average value: 1.83 J/cm² Grade Count:25 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 1105-7741 PEEK, with mineral filler, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | |
Idemitsu Kosan Xarec® EA 537 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications |
|||
Charpy Impact, Notched | <= 1.00 J/cm² @Temperature 23.0 °C |
<= 4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Lanxess Durethan® DP BM 410 H2.0 901510 Nylon 6, 10% Mineral + Glass Fiber PA 6, injection molding grade, 10% glass fibers/mineral, good heat-ageing resistance |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 1104/XCF/30 Polyether ketone, with carbon fiber, easy flowing Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL SE0 PPE+HIPS (Europe-Africa-Middle East) NORYL SE0 is an unfilled, flame retardant material with a Vicat B/120 of 130C according ISO 306. NORYL SE0 is V0 at 1.6 mm according UL94 and halogen free according VDE/DIN 472 part 815. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | 80*10*4mm, Cut; ISO 179/1eA |
SABIC Innovative Plastics SABIC PPCOMPOUND G3220A PP SABIC® PPcompound G3220A is a general purpose, 20% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS is 209767996. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA), 33% Glass Fiber Amodel® AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® 1SBVX-50H LDS black PA1010-GF50 Product Description: Grilamid 1SBVX-50H LDS black is a 50% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is specifically optimized for the laser Direct Structuring techno.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® EBGM-30 HX PA666-GF30 Product description: Grilon EBGM-30 HX is a specially heat stabilized PA66+PA6 injection molding grade with 30% glass fibers. Grilon EBGM-30 HX has the following important properties: High heat resi.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Stanyl® TW200F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 GV 25 DCHP 25% Glass Fiber Nylon 66, Special Heat Ageing Stabilization, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 GV 25 HWCP 25% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® HT2VZ-33H PA6T/66-GF33 Product description: Grivory HT2VZ-33H is a 33% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT2VZ-33H is an injecti.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 30.0 °C |
4.76 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSGZ-30 PA666-GF30 Product description: Grilon TSGZ-30 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSGZ-30 has the following important p.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 30.0 °C |
4.76 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4106 nat PA612-GF30 Product description: Grilamid XE 4106 natural is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorptiong.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® BK-30 PA6-GB30 Information provided by EMS Grivory |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addinyl A2I V25 Flame Retardant Nylon 66, 25% Glass Filled Flame retardant, 25% glass fiber reinforced, halogen freeInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO 179/IeA |
Addiplast Addilene J 430 N30 Polypropylene Copolymer Good surface appearanceInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® S-114 PPS Resin Glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group) |