Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.150 - 0.250 J/cm² | 0.714 - 1.19 ft-lb/in² | ISO 179/1eA |
Raschig Group EN 5007 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Charpy Impact, Notched | 0.150 - 0.250 J/cm² | 0.714 - 1.19 ft-lb/in² | Injection; ISO 179/1eA |
Raschig Group RALUPOL® 2100 UP Polyester Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta.. |
|||
Charpy Impact, Notched | 0.150 - 2.40 J/cm² | 0.714 - 11.4 ft-lb/in² | Average value: 1.20 J/cm² Grade Count:40 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Charpy Impact, Notched | 0.150 - 0.450 J/cm² | 0.714 - 2.14 ft-lb/in² | Average value: 0.211 J/cm² Grade Count:32 |
Overview of materials for Phenolic, Novolac, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ PF 31.5 Phenolic Formaldehyde Resin, Improved Electrical Properties
(discontinued **) Phenolic molding compound, mainly organically filled, electrically high grade, standardized molding compound.Application areas: Parts for electrical and telecommunications technology, car electronic.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ PF 85 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, average notched impact strength, UL listed molding compound 1.5 mm/HB (BK, BN).Application areas: Switch covers, rolls, .. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ PF 2137 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof
(discontinued ** Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, minimal distortion, dish washer proof.Application areas: Iron heat shields, fittings f.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ PF 2535 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof
(discontinued ** Phenolic molding compound, inorganically/organically filled, average heat resistant, steam resistant, dish washer proof, high surface quality.Application areas: Fittings for ovens and dishwashers, t.. |
|||
Charpy Impact, Notched | 0.150 J/cm² - NB | 0.714 ft-lb/in² - NB | Average value: 0.663 J/cm² Grade Count:40 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/1eA |
FKuR Kunststoff Bio-Flex® S 9533 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -23.0 °C |
0.714 ft-lb/in² @Temperature -9.40 °F |
DIN 53453 |
Global PP-1140-T Polypropylene Homopolymer Description-transparency, high stiffness, high heat resistantApplications-disposable drinkware, thin-walled partsInformation provided by Global Polymers Corporation. |
|||
Charpy Impact, Notched | 0.150 J/cm² | 0.714 ft-lb/in² | |
LATI Larton MDT16-02 PPS Polyphenylene Sulfide (PPS) based compound. Magnetic detectable filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & M.. |
|||
Charpy Impact, Notched | 0.150 J/cm² | 0.714 ft-lb/in² | |
LATI Latigea B01 L/07 Bio-Polymer Bio-Polymer (PLA, PHB, ...) based compound. Wood flour. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1040 K Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1100 H Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1100 L Polypropylene, Injection Molding Grade Injection molded parts, film tape, fibrillated film and monofilaments.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1100 RC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1101 R Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 3200 MC Polypropylene Cast film without slip and blocking agents.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 3240 NC Polypropylene Grade containing nucleating agent for transparent injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 - 2.00 J/cm² @Temperature -30.0 - -20.0 °C |
0.714 - 9.52 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.863 J/cm² Grade Count:43 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Charpy Impact, Notched | 0.150 - 0.500 J/cm² | 0.714 - 2.38 ft-lb/in² | Average value: 0.278 J/cm² Grade Count:9 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1100 VC Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1101 N Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1148 RC Polypropylene Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 - 9.00 J/cm² | 0.714 - 42.8 ft-lb/in² | Average value: 0.657 J/cm² Grade Count:53 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact, Notched | 0.150 - 0.800 J/cm² | 0.714 - 3.81 ft-lb/in² | Average value: 0.405 J/cm² Grade Count:11 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact, Notched | 0.150 J/cm² - NB @Temperature -40.0 - -20.0 °C |
0.714 ft-lb/in² - NB @Temperature -40.0 - -4.00 °F |
Average value: 0.997 J/cm² Grade Count:99 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Charpy Impact, Notched | 0.150 - 0.250 J/cm² | 0.714 - 1.19 ft-lb/in² | ISO 179 |
Vyncolit 3520 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |