Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.480 J/cm²
2.28 ft-lb/in²
ISO 179/1eA
Radici Radilon® ACP300 K (dry) Nylon 66
Heat stabilized mineral filledInformation provided by Radici group.
Charpy Impact, Notched 0.480 - 0.640 J/cm²

@Temperature -30.0 - -30.0 °C
2.28 - 3.05 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.575 J/cm² Grade Count:6
Overview of materials for PCTG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Charpy Impact, Notched 0.480 J/cm²

@Temperature -30.0 °C
2.28 ft-lb/in²

@Temperature -22.0 °F
Eastman Eastar DN102 PCTG Copolyester  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical
Charpy Impact, Notched 0.480 J/cm²
2.28 ft-lb/in²
ISO 179/1eA
Nilit FRIANYL B63 FK 1010 Nylon 6 for injection molding, 10% glass fiber and 10% glass ball reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.480 J/cm²

@Temperature 23.0 °C
2.28 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/1eA
FKuR Kunststoff Fibrolon® F 8530 Biodegradable Wood-Plastic Compound, Fiber Reinforced
FIBROLON® are fiber reinforced compounds. Depending on specific customer requirements either a biodegradable polymer or a polyolefin can be used as the polymeric matrix. With the brand name of F..
Charpy Impact, Notched 0.480 J/cm²
2.28 ft-lb/in²
ISO 179/1eA
Lucite International Diakon® TD542 Toughened Acrylic Compound
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by..
Charpy Impact, Notched 0.480 J/cm²

@Temperature -30.0 °C
2.28 ft-lb/in²

@Temperature -22.0 °F
Eastman Eastar DN001 PCTG Copolyester
ISO data as provided by the manufacturer, Eastman Chemical
Charpy Impact, Notched 0.480 J/cm²

@Temperature 23.0 °C
2.28 ft-lb/in²

@Temperature 73.4 °F
EN ISO 179
Ensinger TECASINT 1021 Polyimide, 15% Graphite Filled (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Charpy Impact, Notched 0.480 J/cm²

@Temperature 23.0 °C
2.28 ft-lb/in²

@Temperature 73.4 °F
EN ISO 179
Ensinger TECASINT 4021 Polyimide, Black, 15% Graphite (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Charpy Impact, Notched 0.480 J/cm²
2.28 ft-lb/in²
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® FE3734 NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612 Zytel FE3734 NC010 is an unreinforced lubricated polyamide 612 resin suitable for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 0.480 J/cm²
2.28 ft-lb/in²
ISO R179
Arkema Group ORGASOL® 2002 D Nat 1 Polyamide 12, Food Contact Approved
Information provided by Arkema Group
Charpy Impact, Notched 0.480 J/cm²

@Temperature -30.0 °C
2.28 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® AESN P20 TL Nylon 12, Flexible Grade (Conditioned)
Designation ISO 1874-PA12-P,EHL,22-005Flexible grade for overmolding. Available colors: natural and white. Light and heat stabilized. No lubricant.Flexibility. Very good ability to overmold Pebax an..
Charpy Impact, Notched 0.480 J/cm²
2.28 ft-lb/in²
Arkema Group Rilsan® AESN Y T6L Nylon 12, MoS2 Filled (Dry)
Designation ISO 1874-PA12,EHLS,22-010,MD05Grade with molybdenum filler for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Low friction coefficient. No need of l..
Charpy Impact, Notched >= 0.480 J/cm²

@Temperature 23.0 °C
>= 2.28 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
AKG Polymers Vision PP PPC BL10004 Polypropylene Copolymer Compound
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin..
Charpy Impact, Notched >= 0.480 J/cm²

@Temperature 23.0 °C
>= 2.28 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
AKG Polymers Vision PP PPC BL5005 Polypropylene Copolymer Compound
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin..
Charpy Impact, Notched >= 0.480 J/cm²

@Temperature 23.0 °C
>= 2.28 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
AKG Polymers Vision PP PPC SK3005 Polypropylene Copolymer Compound
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin..
Charpy Impact, Notched >= 0.480 J/cm²

@Temperature 23.0 °C
>= 2.28 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
AKG Polymers Vision PP PPC TC3005 Polypropylene Copolymer Compound
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin..
Charpy Impact, Notched 0.480 J/cm²
2.28 ft-lb/in²
Arkema Group Rilsan® BESN G9 TL Nylon 11, Graphite Filled (Conditioned)
Designation ISO 1874-PA11,EHLS,18-010,CD10Grade with graphite filler for tubes extrusion. Available color: steel gray. Light and heat stabilized.No need of lubricant. Low friction coefficient. Good ..
Charpy Impact, Notched 0.480 J/cm²

@Temperature -30.0 °C
2.28 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® MB 3000 Nylon 11, Sheathing Grade (Conditioned)
Designation ISO 1874-PA11,MF,12-010Polyvalent rigid grade for injection molding and sheathing of cables. Available color: natural. Flame retardant agent, halogen free. Fire-resistant. Easy to be pro..
Charpy Impact, Notched 0.480 J/cm²

@Temperature 23.0 °C
2.28 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® FE3734 NC010 Nylon 612  (Unverified Data**)
Zytel® FE3734 NC010 is an unreinforced, lubricated polyamide 612 resin suitable for injection molding.Information provided by DuPont Performance Polymers