Material Notes:
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineering, Construction, Horticulture, ElectronicsInformation provided by AKG Polymers BV
Physical Properties Metric English Comments
Density 0.900 - 0.920 g/cc
0.0325 - 0.0332 lb/in³
Internal
Filler Content <= 3.0 %
<= 3.0 %
Internal
Melt Flow 26 - 34 g/10 min

@Load 2.16 kg,
Temperature 230 °C
26 - 34 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 65 - 69
65 - 69
Internal
Flexural Modulus >= 1.00 GPa
>= 145 ksi
ISO 178
Charpy Impact, Notched >= 0.480 J/cm²

@Temperature 23.0 °C
>= 2.28 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Falling Dart Impact >= 3.43 J

@Temperature 23.0 °C
>= 2.53 ft-lb

@Temperature 73.4 °F
Internal
Descriptive Properties Value Comments
Application Area horticulture
Color Terracotta
Non-virgin Polymer Content (%), Min 95
Process injection moulding