Ensinger TECASINT 4021 Polyimide, Black, 15% Graphite (PI)

Category Polymer , Thermoplastic , Polyimide, Thermoplastic , Thermoplastic Polyimide, Graphite Filled
Manufacturer Ensinger
Trade Name TECASINT
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Ensinger TECASINT 4021 Polyimide, Black, 15% Graphite (PI).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excellent wear resistance among other things. The TECASINT 2000 series offers these enhanced thermal properties along with lower moisture absorption, a higher degree of toughness, and better machining properties. TECASINT 2011 is unfilled, while TECASINT 2021 contains 15% graphite which offer improved wear resistance and a lower coefficient of friction. TECASINT 2000 series with their superior physical properties, are ideal for application in the aerospace, nuclear, automotive, electrical/electronics, and chemical processing industries.Main features: Very high temperature and oxidative resistance, high creep resistant, good radiation-resistance, good sliding properties, very high chemical resistance, very low absorption of water, flame retardant according to UL94 V-0, not electrically insulating, easily machined, sensitive to hydrolysis in higher thermal rangeApplications: Mechanical engineering, automotive engineering, conveyor technology, hot glass technology, precision engineeringPreferred Fields: Valve seats, friction rings, skid rails, chain guides, piston rings, gripper for hot glass, washers, bearingsInformation Provided by Ensinger Sintimid
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
DIN 53 479
Water Absorption 0.080 %

@Temperature 23.0 °C
0.080 %

@Temperature 73.4 °F
24 hours in water; EN ISO 62
0.53 %

@Temperature 80.0 °C
0.53 %

@Temperature 176 °F
24 hours in water; EN ISO 62
Mechanical Properties Metric English Comments
Hardness, Shore D 86

@Temperature 23.0 °C
86

@Temperature 73.4 °F
DIN 53 505
Tensile Strength 93.0 MPa

@Temperature 23.0 °C
13500 psi

@Temperature 73.4 °F
EN ISO 527
Elongation at Break 3.0 %

@Temperature 23.0 °C
3.0 %

@Temperature 73.4 °F
EN ISO 527
Elongation at Yield 3.4 %

@Temperature 23.0 °C
3.4 %

@Temperature 73.4 °F
Flexural Elongation; EN ISO 178
Tensile Modulus 4.943 GPa

@Temperature 23.0 °C
716.9 ksi

@Temperature 73.4 °F
EN ISO 527
Flexural Strength 131 MPa

@Temperature 23.0 °C
19000 psi

@Temperature 73.4 °F
EN ISO 178
Flexural Modulus 4.93 GPa

@Temperature 23.0 °C
715 ksi

@Temperature 73.4 °F
EN ISO 178
Compressive Yield Strength 163 MPa

@Strain 10.0 %,
Temperature 23.0 °C
23600 psi

@Strain 10.0 %,
Temperature 73.4 °F
EN ISO 604
Compressive Strength 208 MPa

@Temperature 23.0 °C
30200 psi

@Temperature 73.4 °F
EN ISO 604
Compressive Modulus 2.067 GPa

@Temperature 23.0 °C
299.8 ksi

@Temperature 73.4 °F
EN ISO 604
Charpy Impact Unnotched 2.44 J/cm²

@Temperature 23.0 °C
11.6 ft-lb/in²

@Temperature 73.4 °F
EN ISO 179
Charpy Impact, Notched 0.480 J/cm²

@Temperature 23.0 °C
2.28 ft-lb/in²

@Temperature 73.4 °F
EN ISO 179
Compression Set 36 %

@Temperature 23.0 °C
36 %

@Temperature 73.4 °F
Compression at Break; EN ISO 604
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 260 °C
500 °F
DMTA