Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 49.0 MPa | 7110 psi | |
Multibase Multi-Flex® TPE A 8103 BLK Multi-Flex® A 8103 is a moderately low price TPE that has a god tensile and tear strength as well as very good elasticity. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Flexural Strength | <= 49.0 MPa | <= 7110 psi | ISO 178 |
Polykemi AB POLYfill PPC T12020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 49.0 MPa | <= 7110 psi | ISO 178 |
Polykemi AB POLYfill PPC T16020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 49.0 MPa | 7110 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP CZL36 PS LNP LUBRICOMP* CZL36 is a compound based on Polystyrene resin containing 30% Milled Glass and 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | <= 49.0 MPa | <= 7110 psi | ISO 178 |
Polykemi AB POLYfill PPC T8020 FC Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 49.0 MPa | 7110 psi | 3.5%; ISO 178 |
GEHR Plastics ECTFE Polyethylene Chlorotrifluoroethylene Ethylene-Chlortrifluorethylene exhibits an extraordinary impact strength at temperatures ranging from -76°C to 150°C. A great part of the product properties attributes to the very smooth surfa.. |
|||
Flexural Strength | 49.0 MPa | 7110 psi | ASTM D790 |
LG Chemical LUPOL HG-3200 High Gloss Polypropylene, 20% Mineral Fillers LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Flexural Strength | 49.0 MPa | 7110 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS (Europe-Africa-Middle East) LNP* Stat-Loy* A30009 is a compound based on Acrylonitrile Butadiene resin, containing Proprietary Filler, Flame Retardant. Added features include : Permanent Antistatic, Flame retardant. |
|||
Flexural Strength | 49.0 MPa | 7110 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY A3000TXB ABS LNP* STAT-LOY* A3000TXB is a compound based on ABS resin. Added features of this material include: Antistatic, Transparent, Formulated with FDA Food Contact Additives and Bioassessed to ISO 10993... |
|||
Flexural Strength | 49.0 MPa | 7110 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GC-0770 H ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 49.0 MPa | 7110 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® NT-7310 ABS, Unreinforced FR Flame-retardant ABS that can be used in printer frames etc.Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 49.0 MPa | 7110 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SD-0170 F ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 49.0 MPa | 7110 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GC-0770 H ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 49.0 MPa | 7110 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® NT-7310 ABS, Unreinforced FR Flame-retardant ABS that can be used in printer frames etc.Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 49.0 MPa | 7110 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY K3000Z Acetal LNP* STAT-LOY* K3000Z is a compound based on unfilled Acetal resin. Added feature of this material is: Antistat. |
|||
Flexural Strength | 49.0 MPa @Thickness 3.20 mm |
7110 psi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SH 2114 High Impact Polystyrene Characteristics Very high impact strength Easy processing High heat Processing Extrusion MoldingApplications Toys, shoe heels, cosmetic boxes, pill vials Luggage cases Blending with clear polys.. |
|||
Flexural Strength | 49.0 MPa @Thickness 3.20 mm |
7110 psi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 265 Toughened Polystyrene CharacteristicsGood clarity High dart impact strength High heat resistance Good stiffnessProcessing Extrusion Vacuum forming Applications Disposable glasses & bowls Deep draw formed products Ther.. |
|||
Flexural Strength | 49.0 MPa @Thickness 3.20 mm |
7110 psi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP6489 9940 High Impact Polystyrene Characteristics High flow Good toughness Available in black only Processing Injection moldingApplications TV and audio-video back and front cover Material Status: Commercial : ActiveAgency Ratings.. |
|||
Flexural Strength | 49.0 MPa | 7110 psi | ASTM D790 |
SABIC Innovative Plastics NORYL PX2795 PPE+HIPS (Asia Pacific) PPE/HIPS, unfilled, FR-V1, 85 oC |
|||
Flexural Strength | 49.0 MPa | 7110 psi | ISO 178 |
Unitika A1030JR PA6, Conditioned Information provided by Unitika Ltd. |
|||
Flexural Strength | 49.0 MPa | 7110 psi | cond; ISO 178 |
DSM Novamid® 1010C2 PA6 Easy Molding Grade |
|||
Flexural Strength | 49.0 MPa @Temperature 260 °C |
7110 psi @Temperature 500 °F |
ASTM D790 |
Daelim H&L Plavis-G15 DF 15% Graphite Filled Aromatic Polyimide Bearing Direct Formed. Plavis-G-15: Graphite 15 wt% filled, Self lubricating grade for wear and friction applications.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 ca.. |
|||
Flexural Strength | 49.0 MPa | 7110 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336T10L1 Talc Reinforced |
|||
Flexural Strength | 49.0 MPa | 7110 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336T20L1 Talc Reinforced |
|||
Flexural Strength | 49.0 MPa | 7110 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336T30L1 Talc Reinforced |
|||
Flexural Strength | 49.0 MPa | 7110 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336T40L1 Talc Reinforced |
|||
Flexural Strength | 49.0 MPa | 7110 psi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 152 Polypropylene, Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 49.0 MPa @Thickness 3.20 mm |
7110 psi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP6409 High Gloss Polystyrene Characteristics High gloss in co-extrusion Improved dart impact strength of co-extruded sheets Processing Co-extrusion cap layer Applications Gloss cap layer for refrigerator liner and other formin.. |
|||
Flexural Strength | 49.0 MPa | 7110 psi | 0.5 in/min; ASTM D790 |
Ineos Nova Zylar® 94-580-A High Performance Styrenic, Acrylic Copolymer
(discontinued **) Excellent heat distortion temperature, High clarity, strength and toughness, Enhanced mold releaseApplications: Industrial covers and housings, Paper towel dispenser covers, Appliance partsInjection.. |