Ineos Nova Zylar® 94-580-A High Performance Styrenic, Acrylic Copolymer  (discontinued **)

Category Polymer , Thermoplastic , Acrylic (PMMA) , Polystyrene (PS)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos Nova Zylar® 94-580-A High Performance Styrenic, Acrylic Copolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Excellent heat distortion temperature, High clarity, strength and toughness, Enhanced mold releaseApplications: Industrial covers and housings, Paper towel dispenser covers, Appliance partsInjection Speed: Slow to ModerateCharacteristic property data is based on tests of clear or crystal material. Colored material may differ in some properties. All molded samples were an 1/8 thick unless noted.General information about ZYLAR®: ZYLAR® acrylic copolymers are The Clear Alternative to polycarbonate, PETG, impact acrylic and clear ABS for applications that demand clarity and toughness and enhanced processing productivity. ZYLAR is a cost effective alternative in injection molding applications, with over 15 years of proven performance.ZYLAR has proven performance in a variety of applications, including medical, floor care, appliances, consumer goods, office accessories and supplies, pens and mechanical pencils, commercial paper towel dispensers, point of purchase displays, cosmetics packaging, toys, electronics packaging, housewares, consumer & industrial, and other applications.ZYLAR® acrylic copolymers provide value through enhanced performance, manufacturing productivity, ease of processing, and potential for capital avoidance through utilization of existing (styrenics) equipment and tooling.Performance Attributes: Crisp clarityOutstanding practical toughness and ductilityBalance of toughness and clarity Easily decorated Can be printed, hot stamped or metalized.Gamma, Eto and E-beam sterilizableCan be bonded to flexible PVCAlcohol and lipid resistanceResistance to most industrial and commercial cleanersResistance to most household cleanersResistant to most food additivesResidential dishwasher safe - top rackSecondary operations include sonic welding, hotplate welding, ultrasonic bonding and adhesive bondingOver-molding capabilityProduct CapabilitiesAntistatic and indoor UV grades availableAvailable in natural and pre-coloredColor matching capabilitiesCustomer Productivity & Processing5 to 25% density advantage means more parts per pound of resinFaster cycle timeReduced energy and labor costs associated with processing Lower processing temperatures by as much as 150FNo drying Styrenic processingBetter thermal stabilityMore usable regrind and no black specsProduct consistency, color consistency Easily colored at the pressEasy flowAble to utilize existing tooling for PC, clear ABS, impact acrylic, PETG, polyesters, propionate (CAP), PVC and other polymersInformation provided by NOVA Chemicals.INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Water Absorption 0.10 %
0.10 %
24 hrs; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Melt Flow 5.6 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.6 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 61
61
ASTM D785
Tensile Strength, Yield 31.0 MPa
4500 psi
0.2 in/min; ASTM D638
Elongation at Break 53 %
53 %
0.2 in/min; ASTM D638
Modulus of Elasticity 2.34 GPa
339 ksi
0.2 in/min; ASTM D638
Flexural Strength 49.0 MPa
7110 psi
0.5 in/min; ASTM D790
Flexural Modulus 2.07 GPa
300 ksi
0.5 in/min; ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
190 °F
Annealed; ASTM D648
Vicat Softening Point 99.0 °C
210 °F
ASTM D648
Optical Properties Metric English Comments
Refractive Index 1.56
1.56
ASTM D542
Haze 3.1 %
3.1 %
ASTM D1003
Transmission, Visible 87.5 %
87.5 %
ASTM D1003
Processing Properties Metric English Comments
Processing Temperature <= 238 °C
<= 460 °F
Rear Barrel Temperature 179 - 213 °C
354 - 415 °F
Middle Barrel Temperature 185 - 218 °C
365 - 424 °F
Front Barrel Temperature 191 - 224 °C
376 - 435 °F
Melt Temperature 204 - 238 °C
399 - 460 °F
Mold Temperature 27.0 - 54.0 °C
80.6 - 129 °F
Drying Temperature 68.0 °C
154 °F
Dry Time 2 hour
2 hour