| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.52 g/cc | 0.0549 lb/in³ | ASTM D792 |
| 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 | |
| Moisture Absorption | 0.0300 % | 0.0300 % | 50% RH, 24 hrs; ASTM D570 |
| 0.0900 % | 0.0900 % | 23°C / 50% RH; ISO 62 | |
| Linear Mold Shrinkage, Flow | 0.0020 - 0.0030 cm/cm @Time 86400 sec |
0.0020 - 0.0030 in/in @Time 24.0 hour |
ASTM D955 |
| 0.0024 - 0.0026 cm/cm @Time 86400 sec |
0.0024 - 0.0026 in/in @Time 24.0 hour |
ISO 294 | |
| Linear Mold Shrinkage, Transverse | 0.0031 - 0.0037 cm/cm @Time 86400 sec |
0.0031 - 0.0037 in/in @Time 24.0 hour |
ISO 294 |
| 0.0030 - 0.0040 cm/cm @Time 86400 sec |
0.0030 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 21.0 MPa | 3050 psi | ISO 527 |
| 24.0 MPa | 3480 psi | ASTM D638 | |
| Tensile Strength, Yield | 22.0 MPa | 3190 psi | ISO 527 |
| 24.0 MPa | 3480 psi | ASTM D638 | |
| Elongation at Break | 2.3 % | 2.3 % | ASTM D638 |
| 3.5 % | 3.5 % | ISO 527 | |
| Elongation at Yield | 1.6 % | 1.6 % | ISO 527 |
| 1.7 % | 1.7 % | ASTM D638 | |
| Tensile Modulus | 2.55 GPa | 370 ksi | 50 mm/min; ASTM D638 |
| 3.88 GPa | 563 ksi | 1 mm/min; ISO 527 | |
| Flexural Strength | 49.0 MPa | 7110 psi | ISO 178 |
| 52.0 MPa | 7540 psi | ASTM D790 | |
| Flexural Modulus | 4.89 GPa | 709 ksi | ASTM D790 |
| 5.11 GPa | 741 ksi | ISO 178 | |
| Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 7.00 kJ/m² | 3.33 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 2.00 J | 1.48 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 64.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 65.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 67.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 67.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.5 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 83.0 °C | 181 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 83.0 °C @Thickness 3.20 mm |
181 °F @Thickness 0.126 in |
unannealed; ASTM D648 |