Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 30.0 MPa | 4350 psi | |
Plastcom SLOVALEN PC 78 FRT 5 PP, glass fibre, mod. of mech. properties FeaturesModified copolymer PP for injection moulding, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Increased strength in comparison with unfilled.. |
|||
Flexural Strength | 30.0 - 60.0 MPa | 4350 - 8700 psi | ASTM D790 |
Raschig Group PiMC 1241 Sanitary, uni color PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Flexural Strength | <= 30.0 MPa | <= 4350 psi | ISO 178 |
Polykemi AB POLYfill PP EVR8025H UV Polypropylene/EDPM, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 30.0 MPa @Temperature 90.0 °C |
4350 psi @Temperature 194 °F |
ASTM D790 |
Nilit Polynil® P50L Externally Lubricated Nylon 66 Description: Polynil P50L is a general purpose injection molding grade that is widely used for gears, bearings, fasteners, clips. It is also suited for monofilament extrusion.Key characteristics: Ex.. |
|||
Flexural Strength | 30.0 MPa @Temperature 65.0 °C |
4350 psi @Temperature 149 °F |
ASTM D790 |
BASF Capron® 8200 NL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Strength | 30.0 MPa @Temperature 65.0 °C |
4350 psi @Temperature 149 °F |
ASTM D790 |
BASF Capron® 8202 NL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Strength | 30.0 MPa @Temperature 22.0 °C |
4350 psi @Temperature 71.6 °F |
25 mm wide 100 mm long, flat samples; ISO 14125 |
Menzolit Menzolit® MMC 1600 Unsaturated Polyester UP MMC 1600 is a mineral moulding compound (similar to DMC/BMC) providing of a stone like appearance eg. granite or marble. Chrome plated mould surfaces are required. It is recommended that product thi.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Solvay TECHNYL® C 402 M PA6, Conditioned Description: Unreinforced polyamide PA6, high viscosity, containing monomer, for extrusion.Available in: Europe and North AmericaProduct Applications: It is suitable for applications requiring high .. |
|||
Flexural Strength | 30.0 MPa @Temperature 23.0 °C |
4350 psi @Temperature 73.4 °F |
2mm/min; 80x10x4mm; ISO 178 |
SYNTHOS Krasten® FB28 High Impact Polystyrene And Polyethylene Blend Polymer blend HIPS/PE. High toughness, very good tensile properties and environmental stress cracking resistance. Processed mainly by extrusion and thermoforming. Production of sheets and films, tec.. |
|||
Flexural Strength | >= 30.0 MPa | >= 4350 psi | Index |
Shandong Guangyin PA 612 Nylon Resin Features and Applications: As one kind of nylon with better tenacity, PA612 is mainly applicable to coating of high-grade toothbrush monofilaments, monofilaments and cables.Information provided by S.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM D790 |
A. Schulman POLYFORT™ PP 3702 Clarified Copolymer Polypropylene DescriptionPolyfort® PP 3702 is a clarified copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | Olsen; ASTM D747 |
UBE Z322 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Unitika A1030TF PA6, Conditioned Lubricating nylonInformation provided by Unitika Ltd. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | GB/9341 |
Zhejiang Juner JEPP2007 PP For Automotive Parts Applications: Inner Decorate PartsInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3707 CAC03 Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 3707 is a 20% CAC03 filled homopolymer polypropylene product.Information provided by A. Schulman. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3707 CAC03 Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 3707 is a 20% CAC03 filled homopolymer polypropylene product.Information provided by A. Schulman. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM D790 |
A. Schulman POLYFORT™ PP 3702 Clarified Copolymer Polypropylene DescriptionPolyfort® PP 3702 is a clarified copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Borealis Daplen™ EE189AI Polypropylene TPO Compound Daplen™ EE189AI is a 15% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. .. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Polyram PlusTek PD120BK11 Nylon 12 for Extrusion, UV Stabilized Nylon 12 UV stabilized for extrusion application.Information provided by Polyram. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Eurostar Starflam M10009XP PP, Flame Retardant, Injection Molding Starflam M10009XP is an Unfilled Flame Retardant Polypropylene (Copolymer) Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM D790 |
Aclo Accucomp Polypropylene CPO402V Automotive Approved Copolymer Extrusion Grade |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, Conditioned Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Flexural Strength | 30.0 MPa @Temperature 65.0 °C |
4350 psi @Temperature 149 °F |
ASTM Test |
BASF Ultramid® 8202 HS PA6 (Dry) Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab.. |
|||
Flexural Strength | 30.0 MPa @Temperature 65.0 °C |
4350 psi @Temperature 149 °F |
ASTM Test |
BASF Ultramid® 8202C HS PA6 (Dry) Ultramid 8202C HS is a heat stabilized, low viscosity, PA6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It is also.. |
|||
Flexural Strength | 30.0 MPa @Temperature 93.0 °C |
4350 psi @Temperature 199 °F |
ASTM Test |
BASF Ultramid® HPN 9362 40% Mineral Filled PA6 (Conditioned) Ultramid HPN 9362 is a 40% mineral reinforced, impact modified nylon 6 injection molding compound. It is one of the High Productivity Nylon series having improved surface appearance while reducing c.. |
|||
Flexural Strength | 30.0 MPa @Temperature 120 °C |
4350 psi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® HPN 9362 40% Mineral Filled PA6 (Dry) Ultramid HPN 9362 is a 40% mineral reinforced, impact modified nylon 6 injection molding compound. It is one of the High Productivity Nylon series having improved surface appearance while reducing c.. |
|||
Flexural Strength | 30.0 MPa @Temperature 93.0 °C |
4350 psi @Temperature 199 °F |
ASTM Test |
BASF Ultramid® HPN 9362 40% Mineral Filled PA6 (Dry) Ultramid HPN 9362 is a 40% mineral reinforced, impact modified nylon 6 injection molding compound. It is one of the High Productivity Nylon series having improved surface appearance while reducing c.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, DAM Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, Conditioned Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, .. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM D790 |
Teknor Apex Sinpolene CPP2030 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 30% Filler by Weight Features: Copolymer Uses: Automotive Applications; Industrial Applicati.. |