Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYFORT™ PP 3702 Clarified Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer A. Schulman, Inc.
Trade Name POLYFORT™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ PP 3702 Clarified Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DescriptionPolyfort® PP 3702 is a clarified copolymer polypropylene.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Melt Flow 5.0 g/10 min
5.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 69
69
ASTM D785
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638
Flexural Strength 30.0 MPa
4350 psi
ASTM D790
Flexural Modulus 0.953 GPa
138 ksi
ASTM D790
Izod Impact, Notched 4.35 J/cm
8.15 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 51.0 °C
124 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
183 °F
ASTM D648
Users viewing this material also viewed the following: