Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 71.7 MPa | 10400 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 86110 white 1275 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 72.0 MPa | 10400 psi | STN EN ISO 178 |
Plastcom PLASTAMID® 610 BT N 32 C PA610 Basic type PA610 for injection molding, modified for general use. Use: extrusion, filaments, injection molding. Delivered in the natural color.Information Provided by Plastcom spol. s r.o. |
|||
Flexural Strength | 72.0 MPa | 10400 psi | ASTM D790 |
Premix Premi-Glas® 1100-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-10 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
Flexural Strength | 71.7 MPa | 10400 psi | ASTM D790 |
Niche Polymer PA66HIN Nylon 66, High Impact Information provided by Niche Polymer |
|||
Flexural Strength | 72.0 - 77.0 MPa | 10400 - 11200 psi | ASTM D790 |
Proto3000 Accura® 50 Plastic Stereolithography (SLA) Prototyping Polymer Simulate the properties and appearance of molded ABS with this durable, accurate and versatile plastic.Features:Durable and stiffOutstanding accuracy w/out shrinkage related distortionChoice of grey.. |
|||
Flexural Strength | 72.0 MPa | 10400 psi | ISO 178 |
Nilit FRIANYL A63 S Nylon 6.6 for injection molding Nylon 6.6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 72.0 MPa | 10400 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DI001L PC LNP* LUBRICOMP* DI001L is a compound based on Polycarbonate resin containing 2% Silicone. Added characteristics of this grade are: Low Extractable. |
|||
Flexural Strength | 71.7 MPa | 10400 psi | ASTM D790 |
Ravago Manufacturing Americas Enviramid™ N1300THL BK Post Consumer Recycle Nylon 66 Impact Modified, Heat Stabilized, Lubricated, Black and Made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Flexural Strength | 72.0 MPa | 10400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP CG006 PS (Europe-Africa-Middle East) LNP* Lubricomp* CG006 is a compound based on Polystyrene resin containing Graphite. |
|||
Flexural Strength | 72.0 MPa | 10400 psi | 2mm/min; ASTM D790 |
Kingfa HR-527B Modified ABS Features:UL94 HB @ 1.5-3.2mmExcellent heat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd... |
|||
Flexural Strength | 72.0 MPa | 10400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DP002 PC (Europe-Africa-Middle East) LNP* Lubricomp* DP002 is a compound based on Polycarbonate resin containing PTFE and Silicone. Added features of this material include: Internally Lubricated, Easy Molding. |
|||
Flexural Strength | 72.0 MPa | 10400 psi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp ZI001 PPO LNP* Lubricomp ZI001 is a compound based on Modified PPO containing Silicone. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 72.0 MPa | 10400 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON EX02598C PEI LNP* STAT-KON* EX02598C is a compound based on Polyetherimide containing Proprietary Filler(s). Added features of this material include: Clean Compound System, Electrically Conductive. |
|||
Flexural Strength | 72.0 MPa | 10400 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP KZ001L Acetal Copoly LNP* THERMOCOMP* KZ001L is a compound based on Acetal Copolymer resin containing 5% Milled Glass. Added features of this material include: Low Extractible. |
|||
Flexural Strength | 72.0 MPa | 10400 psi | ISO 178 |
Styrolution Polystyrol 143 E GR 2 PS Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b.. |
|||
Flexural Strength | 72.0 MPa | 10400 psi | ISO 178 |
Styrolution Polystyrol 143 E GR 21 PS Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b.. |
|||
Flexural Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP NX07354P PC+ABS (Asia Pacific) This is a PC/ABS compound with improved plating performance, a good candidate for Laser Direct Structuring applications. |
|||
Flexural Strength | 72.0 MPa | 10400 psi | 3-point, 2 mm/min; ISO 178 |
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided .. |
|||
Flexural Strength | 72.0 MPa | 10400 psi | |
Sumitomo Bakelite Durez® 156 Phenolic, Compression Grade Durez 156 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits excellent dimensional stability, high heat resistance, good molded appearance, and UL.. |
|||
Flexural Strength | 71.6 MPa | 10400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® BF-0679P MABS, Unreinforced Scratch Resistant Scratch resistant material that is used for the exterior material of flat TVInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL BN31 PPE+PS Blowmoldable. Excellent processability and flammability. Good heat resistance. Low temperature impact strength. Dimensional stability. |
|||
Flexural Strength | 71.7 MPa | 10400 psi | ASTM D790 |
Chase Plastics CP Pryme® NN100MD2 (COND, 50% RH) Nylon 66 with 2% MoS2 Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 72.0 MPa | 10400 psi | ASTM D790 |
Plenco 3303 Phenolic, Granular, Compression Molded Plenco 03303 is a renumber of Plaslok 5303. Plenco 03303 is a two-stage, mineral and flock-filled phenolic molding compound offering excellent electrical insulating properties. It can be processed b.. |
|||
Flexural Strength | 72.0 MPa | 10400 psi | ASTM D790 |
Unitika M2350 PA6, Conditioned Nano composite nylonInformation provided by Unitika Ltd. |
|||
Flexural Strength | 72.0 MPa | 10400 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3715 Glass Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 3715 is a 15% glass filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Strength | 72.0 MPa | 10400 psi | ISO 178 |
Denka TH-21 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Flexural Strength | 72.0 MPa | 10400 psi | 2 mm/min; ISO 178 |
Chi Mei Polylac® PA-756 ABS - High Flow High rigid, high flow |
|||
Flexural Strength | 72.0 MPa | 10400 psi | ASTM D790 |
Ashley Polymers Ashlene® ABS Resin E213B General purpose, black, utility grade for injection molding with medium gloss.Data provided by the manufacturer |
|||
Flexural Strength | 72.0 MPa | 10400 psi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 602 Nylon 6/6, High Impact Modified Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Flexural Strength | 72.0 MPa | 10400 psi | ISO 178 |
Polyplastics Duracon® NW-02 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |