| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Geon™ Vinyl Rigid Extrusion 86110 white 1275 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 79 | 79 | 15 sec; ASTM D2240 |
| Tensile Strength, Yield | 40.4 MPa | 5860 psi | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 2.79 GPa | 405 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Strength | 71.7 MPa | 10400 psi | ASTM D790 |
| Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 80.4 °C | 177 °F | Annealed; ASTM D648 |
| 78.3 °C @Thickness 3.18 mm |
173 °F @Thickness 0.125 in |
Unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 78.4 °C | 173 °F | Annealed; ASTM D648 |
| 73.4 °C @Thickness 3.18 mm |
164 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Forms | Cube | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Processing Method | Coextrusion | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Capstock | |
| Fencing & Decking | ||
| Outdoor Applications |