| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade |
| Manufacturer | Niche Polymer |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Niche Polymer PA66HIN Nylon 66, High Impact.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage | 0.0180 cm/cm | 0.0180 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 52.4 MPa | 7600 psi | ASTM D638 |
| Elongation at Break | 65.0 % | 65.0 % | ASTM D638 |
| Flexural Strength | 71.7 MPa | 10400 psi | ASTM D790 |
| Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
| Izod Impact, Unnotched | 8.54 J/cm @Thickness 3.17 mm |
16.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 70.0 °C | 158 °F | ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 249 - 260 °C | 480 - 500 °F | ASTM D789 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Natural |